Monel Alloy NO 5500 Pipe
As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.
- Send E-mail: ss@gneesteel.com
Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of monel alloy no 5500 pipe in China. If you're going to wholesale high quality monel alloy no 5500 pipe made in China, welcome to get free sample from our factory. Good service and reasonable price are available.
Monel Alloy NO5500 pipe is a type of pipe made from a high-performance nickel-copper alloy known for its exceptional corrosion resistance and increased strength compared to other similar alloys. This alloy, marketed under the name "Monel® K-500" by the Special Metals Corporation group of companies, is identified as UNS N05500. What sets it apart is its composition and the process involved in enhancing its properties. The addition of aluminum and titanium to the nickel-copper base, coupled with heating under controlled conditions, results in the precipitation of Ni3(Ti, Al) submicron particles throughout the matrix. This process not only retains the excellent corrosion resistance of traditional Monel alloys but also significantly boosts its strength and hardness.
MECHANICAL PROPERTIES
|
Condition |
Yield strength Rp0.2, |
Tensile strength Rm, |
Elongation |
Hardness |
Impact, Charpy-V, -32ºC |
Pre |
|
|
H 900 |
≥ 1170 |
≥ 1310 |
≥ 8 |
≤ 440 |
≥ 17 |
||
|
H 1075 |
≥ 860 |
≥ 1000 |
≥ 10 |
≤ 375 |
≥ 27 |
≥ 17 |
|
|
H 1150 |
≥ 725 |
≥ 930 |
≥ 16 |
≤ 352 |
≥ 27 |
≥ 17 |
|
|
DH 1150 |
≥ 725 |
≥ 860 |
≥ 16 |
≤ 311 |
≥ 27 |
≥ 17 |
Monel Alloy NO 5500 Forged Fittings Dimensions :
| Size Of Pipes In Inch | Dia Of (A) |
Dia. Of (B) |
ASME B16.11 Weight in Pounds |
|---|---|---|---|
| 1/8 | 0.69 | 0.66 | 0.06 |
| 1/4 | 0.80 | 0.80 | 0.10 |
| 3/8 | 0.94 | 0.97 | 0.15 |
| 1/2 | 1.11 | 1.17 | 0.22 |
| 3/4 | 1.24 | 1.38 | 0.32 |
| 1 | 1.43 | 1.74 | 0.52 |
| 1-1/4 | 1.72 | 2.07 | 0.76 |
| 1-1/2 | 1.87 | 2.36 | 0.99 |
| 2 | 2.25 | 2.86 | 1.49 |
| 2-1/2 | 2.68 | 3.57 | 2.78 |
| 3 | 3.05 | 4.23 | 4.41 |
| 4 | 3.72 | 5.24 | 6.72 |



Hot Tags: monel alloy no 5500 pipe, China monel alloy no 5500 pipe suppliers, surface finish alloy, alloy marketing, alloy dealer, alkali resistant alloy, alloy profit, Monel 500