Alloy steel has higher strength and toughness than carbon steel, and its reinforcement effect with the increace of tissue imbalance and tend to be more obvious, and the strength of the alloy steel annealing state than carbon steel has a lot of advantages, and in normalizing, than obviously increase the carbon steel and the strength of the alloy steel after quenching and tempering, the steel reinforcement effect is the most significant. Some alloy steels have excellent thermal hardness and other special properties, such as heat resistance, corrosion resistance, wear resistance and magnetic properties.
Send Inquiry
Chat Now

As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.

Product Introduction

Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of monel alloy 502 pipe in China. If you're going to wholesale high quality monel alloy 502 pipe made in China, welcome to get free sample from our factory. Good service and reasonable price are available.

 

Monel Alloy 502 pipe is a type of nickel-copper alloy pipe that is known for its excellent corrosion resistance and high strength. It is commonly used in applications where resistance to corrosion and wear is required, such as in the chemical processing, marine, and aerospace industries. Monel Alloy 502 pipe is available in various sizes and thicknesses to meet the specific requirements of different applications.

Physical Properties

The physical properties of Monel 502 are highlighted in the following table.

Properties Metric Imperial
Density 7.7-8.03 g/cm³ 0.278-0.290 lb/in³
Melting point 1330°C 2425°F

Mechanical Properties

The mechanical properties of Monel 502 are outlined in the following table.

Properties Metric Imperial
Tensile strength 1158 MPa 167954 psi
Yield strength 1034 MPa 149969 psi
Elastic modulus 190-210 GPa 27557-30458 ksi
Poisson's ratio 0.27-0.30 0.27-0.30
Elongation 15% 15%
Reduction of area 53% 53%
Hardness 335 335

Thermal Properties

The thermal properties of Monel 502 are displayed in the following table.

Properties Metric Imperial
Thermal conductivity 42.7 W/mK 296 BTU in/hr.ft².°F

 

Monel Alloy 502 pipeMonel Alloy 502 pipeMonel Alloy 502 pipe