Special nickel and precision expansion alloys follow UNS, W.Nr. and GB standards, leading to grade confusion during procurement and MTC checking. This page cross-matches all mainstream grades with three standard codes & density data, supporting drawing alignment, certificate verification and material cost budgeting.

 

Nickel-based Heat & Corrosion Resistant Alloys

 

Commercial Grade UNS No. W.Nr. GB Standard Density (g/cm³)
Alloy 20 N08020 2.4660 NS1403 8.10
Alloy 28 N08028 1.4563 NS1404 8.05
Alloy 59 N06059 2.4605 NS3311 8.60
Hastelloy B N10001 2.4810 NS3201 9.24
Hastelloy B-2 N10665 2.4617 NS3202 9.22
Hastelloy B-3 N10675 2.4600 NS3203 9.22
Hastelloy B-4 N10629 2.4600 NS3204 9.20
Hastelloy C N10002 2.4819 NS3303 8.60
Hastelloy C-4 N06455 2.4610 NS3305 8.60
Hastelloy C-22 N06022 2.4602 NS3308 8.70
Hastelloy C-276 N10276 2.4819 NS3304 8.90
Hastelloy C-2000 N06200 2.4675 NS3405 8.50
Hastelloy G N06007 2.4618 NS3402 8.30
Hastelloy G-3 N06985 2.4619 NS3403 8.14
Hastelloy G-30 N06030 2.4603 NS3404 8.22
Hastelloy G-35 N06035 2.4643 - 8.18
Hastelloy G-50 N06950 - NS3310 8.38
Hastelloy X N06002 2.4665 GH3536 8.23
Inconel 617 N06617 2.4663 - 8.36
Inconel 718 N07718 2.4668 GH4169 8.24
Inconel X-750 N07750 2.4669 GH4145 8.28
Inconel 600 N06600 2.4816 NS3102 8.47
Inconel 601 N06601 2.4851 NS3103 8.11
Inconel 625 N06625 2.4856 NS3306 8.44
Inconel 686 N06686 2.4606 NS3309 8.73
Inconel 690 N06690 2.4642 NS3105 8.19
Inconel 706 N09706 - - 8.05
Incoloy 825 N08825 2.4858 NS1402 8.14
Incoloy 800 N08800 1.4876 NS1101 7.94
Incoloy 800H N08810 1.4958 NS1102 7.94
Incoloy 800HT N08811 1.4959 NS1104 7.94
Incoloy A286 S66286 1.4980 GH2132 7.93
Monel 400 N04400 2.4360 NS6400 8.80
Monel K500 N05500 2.4375 NS6500 8.44
Nickel 200 N02200 2.4066 N5 8.89
Nickel 201 N02201 2.4068 N7 8.89
Waspaloy N07001 2.4654 GH4738 8.20

 

Cross-check drawing grades like Alloy 825, Inconel 718, Hastelloy C276 via this table. Send grade & size to get stock specs, mill certificates and tailored quotations for plates, pipes, bars and forgings.

 

Precision Low Expansion Alloy Grade Chart

 

Beyond high-temp anti-corrosion nickel alloys, Fe-Ni precision expansion alloys serve electronic sealing and instrumentation parts, enabling grade verification for semiconductor, vacuum equipment and glass-to-metal sealing applications.

 

Commercial Grade UNS No. W.Nr. GB Standard Density (g/cm³)
KOVAR K94610 1.3981 4J29 8.30
INVAR K93600 1.3912 4J36 8.10

 

Grade Cross Reference Table Usage Guide:

  • Drawing Matching Quickly convert overseas UNS / W.Nr. designations to domestic GB NS, GH and 4J grades to prevent wrong material orders.
  • MTC Verification Cross-check factory mill certificates against three standard codes to avoid counterfeit or substitute materials.
  • Material Selection Support Standard density data is included for pre-calculation of plate and pipe weight budgets.

 

Get Grade Based Quotation

 

Selected mainstream grades may be available from stock. We offer full services: solution annealing, saw cutting, plasma cutting, NDT inspection, plus EN10204 3.1 / 3.2 certification. Our materials serve chemical, sour oil & gas, offshore and electronic sealing industries.

whatsapp

Phone

E-mail

Inquiry