Monel Alloy 404 Pipe
As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.
- Send E-mail: ss@gneesteel.com
Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of monel alloy 404 pipe in China. If you're going to wholesale high quality monel alloy 404 pipe made in China, welcome to get free sample from our factory. Good service and reasonable price are available.
Monel Alloy 404 pipe is a high-performance nickel-copper alloy pipe with excellent corrosion resistance and good machinability. The alloy is widely used in high temperature and extreme environments due to its unique chemical composition and physical properties. The following is a specific analysis:
Basic composition and ingredients
Main ingredients: Monel Alloy 404 is mainly composed of nickel (Ni) and copper (Cu), which together provide the alloy with high strength and corrosion resistance. In addition, the alloy also contains small amounts of elements such as iron (Fe), manganese (Mn), carbon (C), silicon (Si), aluminum (Al) and sulfur (S).
Chemical composition details: The specific chemical composition includes nickel content between 52.0% and 57.0%, copper constituting the balance, iron content not exceeding 0.5%, manganese content not exceeding 0.1%, carbon content not exceeding 0.15%, silicon content not exceeding 0.1%, aluminum content not exceeding 0.05%, and sulfur content not exceeding 0.024%.
Physical and Mechanical Properties
Density and Melting Point: Monel Alloy 404 has a density of 8.91 g/cm3, which allows it to remain stable in high temperature environments.
Mechanical Properties: Although specific tensile strength, yield strength and elongation data are not provided, it generally has good mechanical strength and ductility based on the characteristics of the alloy.
Environmental Corrosion Resistance
Wide Corrosion Resistance: Monel 404 has good corrosion resistance in slightly oxidizing media environments, neutral environments, and suitable reducing environments. This makes it widely used in fields such as chemistry and petrochemicals.
Monel 404 Plates Equivalent Grades
| STANDARD | WERKSTOFF NR. | UNS |
| Monel 404 | 2.4867 | N04404 |
404 Monel Plates Chemical Composition :
>
| % | Ni | Cu | Fe | C | Mn | Si | S | Al |
| min | 52.0 | balance | – | – | – | – | – | – |
| max | 57.0 | 0.50 | 0.15 | 0.10 | 0.10 | 0.024 | 0.05 |
ASTM F-96 Monel 404 Plates Mechanical Physical Properties:
| Element | Density | Melting Point |
| Monel 404 | 8.91 g/cm3 | 1300-1350ºC |



Hot Tags: monel alloy 404 pipe, China monel alloy 404 pipe suppliers, alloy reuse, alloy drawing, density alloy, alloy development, alloy performance, alloy profit
Previous
Monel Round Bar ASTM B164You Might Also Like
Send Inquiry