Monel Alloy NO5500 Pipe
video

Monel Alloy NO5500 Pipe

MONEL K-500(UNS N05500/W.Nr. 2.4375) alloy has corrosion resistance equivalent to 400, but has higher mechanical strength and hardness. It has good thermal corrosion resistance and long-term structural stability. Mainly used to manufacture turbine blades and gas turbine blades on aero engines whose working temperature is below 750℃; used to manufacture fasteners and springs on ships; pump and valve parts on chemical equipment; scraper blades on papermaking equipment Wait.
Send Inquiry
Chat Now

As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.

Product Introduction

Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of monel alloy no5500 pipe in China. If you're going to wholesale high quality monel alloy no5500 pipe made in China, welcome to get free sample from our factory. Good service and reasonable price are available.

 

Monel Alloy NO5500 seamless pipe is a highly valued material in industries where its unique combination of corrosion resistance, mechanical strength, and weldability is required. Its cost reflects its premium properties and specialized manufacturing processes, but the benefits in terms of durability and longevity often make it a cost-effective choice for demanding applications.

Chemical Composition:

  Cr Ni Mo Co Nb (+Ta) Ti V W Cu C Mn N Si P S Fe Al
Min   63.00       0.35     27.00               2.30
Max           0.85     33.00 0.25 1.50   0.50   0.010 2.00 3.15

Monel K500 Pipes Mechanical Properties

Element Density Tensile Strength Yield Strength (0.2%Offset) Melting Point Elongation
Monel 400 8.8 g/cm3 Psi – 80,000 , MPa – 550 Psi – 35,000 , MPa – 240 1350 °C (2460 °F) 40 %
Monel K500 8.44 g/cm3 Psi – 1,15,000 , MPa – 790 Psi – 1,60,000 , MPa – 1100 1350 °C (2460 °F) 20 %

Monel Alloy NO5500 pipeMonel Alloy NO5500 pipeMonel Alloy NO5500 pipe

Hot Tags: monel alloy no5500 pipe, China monel alloy no5500 pipe suppliers, alloy knowledge, alloy business, alloy heat treatment, brazability alloy, flexible alloy, sulfide resistant alloy