Monel Alloy K-500 Thick-walled Pipe
video

Monel Alloy K-500 Thick-walled Pipe

Monel K-500 thick-walled pipe is a seamless, thick-walled Monel K-500 pipe. Compared with Monel K-500 seamless pipe, it not only inherits high temperature resistance and corrosion resistance, but also has better high pressure resistance. Therefore, Monel K-500 thick-walled tubes are often used in high-pressure equipment. In the manufacturing process, due to the thicker wall thickness, cold rolling and cold drawing processes are no longer applicable, so the Monel K-500 thick-walled pipe is perforated and hot-rolled from Monel K-500 round bar.
Send Inquiry
Chat Now

As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.

Product Introduction

Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of monel alloy k-500 thick-walled pipe in China. If you're going to wholesale high quality monel alloy k-500 thick-walled pipe made in China, welcome to get free sample from our factory. Good service and reasonable price are available.

 

Monel Alloy K-500 Thick-walled Pipe

Product Details

MONEL® alloy K-500 (UNS N05500 / W.Nr. 2.4375) is a nickel-copper alloy which combines the excellent corrosion resistance of MONEL alloy 400 with the added advantages of greater strength and hardness. The increased properties are obtained by adding aluminum and titanium to the nickel-copper base.

Monel K-500 thick-walled pipe is a seamless, thick-walled Monel K-500 pipe. Compared with Monel K-500 seamless pipe, it not only inherits high temperature resistance and corrosion resistance, but also has better high pressure resistance. Therefore, Monel K-500 thick-walled tubes are often used in high-pressure equipment. In the manufacturing process, due to the thicker wall thickness, cold rolling and cold drawing processes are no longer applicable, so the Monel K-500 thick-walled pipe is perforated and hot-rolled from Monel K-500 round bar.

 

Customized Dimensions

Outside Diameter (OD)

10~600

mm

Wall Thickness (THK)

2.5~100

mm

Length (L)

0.5~12

m

The size can be customized according to ASME B36.10 / ASME B36.19

*Customized size please confirm with us

Standards for Monel K-500 Welded Pipe & Tube

DIN 17751

*We will strictly produce Monel K-500 Thick-walled Pipe according to the standard

 

Surface to be Customized

product-1-1

Pickled Surface

product-1-1

Polished Surface

*We can also sandblast the pipes according to your requirements

Chemical Composition of Monel K-500

Data Sheet

Physical Properties

Density g/cm3 8.44
lb/in.3 0.305
Melting Range °F 2400 - 2460
°C 1315 - 1350

Mechanical Properties

Condition & Size Tensile Strength Yield Strength
(0.2% Offset)
Elongation Reduction of Area Hardness
MPa MPa % % Rockwell
Cold-Drawn,Annealed 621-758 276-448 45-25 ... 90B max.
Cold-Drawn,Annealed and Aged 896-1241 586-827 30-15 ... 24-36C
Cold-Drawn,As-Drawn 758-1103 586-965 15-2 ... 95B-32C
Cold-Drawn,As-Drawn, Aged 965-1517 690-1379 25-3 ... 27-40C

Monel K-500 Applications

Springs, pumps, valves, and fasteners.

Monel K-500 Alloy Industries Supplied

Oil & Gas Extraction, Marine, Chemical Processing, and Medical.

Hot Tags: monel alloy k-500 thick-walled pipe, China monel alloy k-500 thick-walled pipe suppliers, alloy weakening, alloy brand awareness, alloy packaging, 502 2 4360 Monel Alloy Pipe And Tube, marine alloy, alloy development

Send Inquiry

whatsapp

Phone

E-mail

Inquiry