Monel Alloy R-405 Round Bar
As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.
- Send E-mail: ss@gneesteel.com
Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of monel alloy r-405 round bar in China. If you're going to wholesale high quality monel alloy r-405 round bar made in China, welcome to get free sample from our factory. Good service and reasonable price are available.
Monel Alloy R-405 Round Bar
Product Details
Standards for Monel R-405 Round Bar & Rod
ASTM B164
ASME SB 164
Federal QQN-281
SAE AMS 4674
SAE AMS 7234
Military MIL-N-894
NACE MR-01-75
*As a professional manufacturer, our default standard for Monel R-405 round bar & rod is ASTM B164. We can also produce according to other standards as per you required.
Data Sheet
Physical Properties
| Density | g/cm3 | 8.8 | |
|---|---|---|---|
| lb/in.3 | 0.318 | ||
| Melting Range | °F | 2370 - 2460 | |
| °C | 1300 - 1350 | ||
Mechanical Properties
| Condition & Size | Tensile Strength | Yield Strength (0.2% Offset) |
Elongation | Reduction of Area | Hardness |
|---|---|---|---|---|---|
| MPa, min | MPa, min | %, min | %, min | Rockwell, max | |
| Cold-worked (as worked or stress-relieved) / under 12.7mm | 585 | 345 | 8 | ... | ... |
| Cold-worked (as worked or stress-relieved) / 12.7mm to 76.2mm, incl | 585 | 345 | 15 | ... | ... |
| Cold-worked (as worked or stress-relieved) / 76.2mm to 101.6mm, incl | 552 | 345 | 15 | ... | ... |
| Hot-worked (as hot-worked or stress-relieved) / 76.2mm and less | 517 | 241 | 30 | ... | ... |
| Hot-worked (annealed) or cold-worked (annealed) / All sizes | 480 | 170 | 35 | ... | ... |
*Mechanical Properties According to ASTM B164