Incoloy 028
video

Incoloy 028

INCOLOY® alloy 028 (UNS N08028/W. Nr. 1.4563) is a highly alloyed austenitic stainless steel offering resistance to a variety of corrosive media. By virtue of its contents of chromium and molybdenum, the alloy offers resistance to both oxidizing and reducing acids and salts. The presence of copper increases its resistance to sulfuric acid. The alloy is used in the chemical and petrochemical processing industry. Alloy tubes are cold worked to high strength levels for downhole service in moderately corrosive deep sour gas wells.
Send Inquiry
Chat Now

As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.

Product Introduction

Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of incoloy 028 in China. If you're going to wholesale high quality incoloy 028 made in China, welcome to get free sample from our factory. Good service and reasonable price are available.

 

INCOLOY® alloy 028 (UNS N08028/W. Nr. 1.4563) is a highly alloyed austenitic stainless steel offering resistance to a variety of corrosive media. By virtue of its contents of chromium and molybdenum, the alloy offers resistance to both oxidizing and reducing acids and salts. The presence of copper increases its resistance to sulfuric acid. The alloy is used in the chemical and petrochemical processing industry. Alloy tubes are cold worked to high strength levels for downhole service in moderately corrosive deep sour gas wells.

Main Standards

ASTM B668

Seamless Pipe & Tube

ASTM B829

Seamless Pipe & Tube

ASTM B709

Plate, Sheet and Strip

Chemical Composition

Data Sheet

Physical Properties

Density g/cm3 8.0
lb/in.3 0.29
Specific Heat Btu/lb-°F 0.105
J/kg-°C 450
Thermal Conductivity at 200°F (93°C) Btu-in/ft2-h-°F 66
W/m-°C 11.4
Electrical Resistivity ohm circ mil/ft 594
μΩ-m 0.99
Young's Modulus (70°F) 103 ksi 29.0
GPa 200

Mechanical Properties

Annealed
Tensile Strength ksi 73
MPa 500
Yield Strength (0.2% Offset) ksi 31
MPa 214
Elongation % 40
Hardness HRB 80-90
Cold Worked
Tensile Strength ksi 130
MPa 896
Yield Strength (0.2% Offset) ksi 110
MPa 758
Elongation % 15
Hardness HRC 33 max.

product-750-750product-750-750product-750-750product-750-750

 

FAQ

Q: How do you control quality ?
A: Mill Test Certification is supplied with shipment, Third Party Inspection is available. and we also get ISO,SGS,Alibaba Verified.
Q: What are the advantages of your company ?
A: We have many professionals, technical personnel, more competitive prices and best after-dales service than other stainless steel companies.
Q: How many coutries you already exported ?
A: Exported to more than 50 countries mainly from America, UK, Kuwait, Egypt, Turkey, Jordan,India, etc.
Q: Can you provide sample ?
A: Yes. We can provide the small samples in stock for free, as long as you contact us.Customized samples will take about 5-7 days.