INCOLOY® alloy 890 (UNS N08890) is the latest addition to the INCOLOY alloy family of heat resistant alloys. Alloy 890 joins the existing INCOLOY products in offering high strength along with excellent resistance to oxidation, carburization, and sulfidation at temperatures up to 2200°F (1200°C).
Send Inquiry
Chat Now

As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.

Product Introduction

Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of incoloy 890 in China. If you're going to wholesale high quality incoloy 890 made in China, welcome to get free sample from our factory. Good service and reasonable price are available.

 

INCOLOY® alloy 890 (UNS N08890) is the latest addition to the INCOLOY alloy family of heat resistant alloys. Alloy 890 joins the existing INCOLOY products in offering high strength along with excellent resistance to oxidation, carburization, and sulfidation at temperatures up to 2200°F (1200°C).

Alloy 890 offers the high chromium content of alloy 803 along with enhanced properties from additions of silicon, molybdenum, and niobium. Alloy 890 is protected by United States Patent Number 5,873,950 dated February 23, 1999.

INCOLOY alloy 890 is a solid-solution, single phase alloy. It is normally supplied in the annealed condition. Annealing alloy 890 is accomplished by heating to a temperature between 2050 and 2200°F (1121 and 1204°C), holding for a time commensurate with section thickness, followed by rapid cooling in air or water quenching. Alloy 890 can be sensitized by carbide precipitation when exposed to intermediate temperatures for extended periods of time. However, sensitization of materials such as alloy 890 which are primarily used at elevated temperatures is not generally considered a significant problem since conditions to cause aqueous corrosion are not often encountered.

Mechanical Properties

INCOLOY alloy 890 is supplied in the annealed condition. The tensile and yield strength values of alloy 890 at ambient and elevated temperatures are approximately the same as those of alloy 803 and slightly higher than values for alloy 800HT®. Like alloy 803 it is strengthened by its content of chromium and carbon. However, alloy 890 is further strengthened, especially at very high temperatures, by molybdenum and niobium.

Corrosion Resistance

By virtue of its chromium and silicon contents, alloy 890 offers the greatest resistance to attack at elevated temperatures of any of the INCOLOY family of alloys. It is seen that alloy 890 outperforms even alloy 803, which is well known for its resistance to attack in carburizing environments. Again, alloy 890 offers significantly superior performance.

More +

Main Standards

ASTM B407

Pipe and Tube

ASTM B408

Rod and Bar

ASTM B409

Plate, Sheet and Strip

ASTM B906

Plate, Sheet and Strip

Chemical Composition

Data Sheet

Physical Properties

Density g/cm3 7.94
lb/in.3 0.287
Melting Range °F 2388 - 2522
°C 1309 - 1383

Mechanical Properties

Product Temper Temperature
°F (°C)
0.2% Yield
Strength, ksi (MPa)
Ultimate Tensile
Strength, ksi (MPa)
Elongation Reduction of
Area, %
Hot-Rolled Plate Solution-Annealed 72 (22) 39.4 (272) 94.5 (652) 46.6 62.7
Cold-Drawn Tubing Solution-Annealed 72 (22) 48.4 (334) 94.2 (652) 46.5 60.1
Hot-Rolled Plate Solution-Annealed 1600 (870) 16.0 (110) 23.5 (132) 84.8 71.0
Hot-Rolled Plate Solution-Annealed 1800 (980) 9.6 (66) 13.4 (92) 98.0 87.5
Hot-Rolled Plate Solution-Annealed 2000 (1100) 6.4 (44) 9.0 (62) 83.6 91.8

More +product-720-720product-720-720product-720-720product-720-720

FAQ

 

Q: How do you control quality ?
A: Mill Test Certification is supplied with shipment, Third Party Inspection is available. and we also get ISO,SGS,Alibaba Verified.
Q: What are the advantages of your company ?
A: We have many professionals, technical personnel, more competitive prices and best after-dales service than other stainless steel companies.
Q: How many coutries you already exported ?
A: Exported to more than 50 countries mainly from America, Russia, UK, Kuwait, Egypt, Turkey, Jordan,India, etc.
Q: Can you provide sample ?
A: Yes. We can provide the small samples in stock for free, as long as you contact us.Customized samples will take about 5-7 days.

Hot Tags: incoloy 890, China incoloy 890 suppliers, alloy for maintenance baths, incoloy alloy metal pipe, alloy for gasket materials, alloy for superconductors, alloy for selective laser sintering baths, alloy for intelligent manufacturing baths

Send Inquiry

whatsapp

Phone

E-mail

Inquiry