UNS N08811 Pipes to their customers. The industry is using superior quality of raw material to manufacture pipes. The industry examines and evaluates each and every pipe in order to detect any defect and other problems while exporting across the globe. Buyers prefer to buy top-notch quality pipes from them. They offer accurate dimensions, high end finishing, durability, reliability and reasonable market price to their customers.
Send Inquiry
Chat Now

As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.

Product Introduction

Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of incoloy alloy uns n08811 pipe in China. If you're going to wholesale high quality incoloy alloy uns n08811 pipe made in China, welcome to get free sample from our factory. Good service and reasonable price are available.

 

Incoloy Alloy UNS N08811 pipe is a nickel iron chromium alloy pipe widely used in high temperature and corrosion resistant environments.
Main ingredients and properties:
Incoloy Alloy UNS N08811 is mainly composed of nickel, iron, and chromium, with molybdenum, copper and other elements added to enhance its specific properties. Nickel, as the main component, provides excellent strength and toughness, while chromium and molybdenum significantly improve the material's resistance to corrosion, especially to oxidizing acids.
This alloy performs particularly well in reducing and oxidizing environments and can resist corrosion from a variety of chemical media, such as sulfuric acid, phosphoric acid, etc.
High temperature and mechanical properties:
Incoloy Alloy UNS N08811 maintains excellent mechanical properties under high temperature conditions, including high tensile and yield strengths, as well as good creep and fatigue resistance, making it an ideal choice for high temperature applications.
The thermal stability of the alloy is particularly excellent. Even if it is exposed to high temperature for a long time, it can maintain stable microstructure and mechanical properties and is not prone to aging or performance degradation.

Physical properties of Incoloy UNS N08811 pipe

Properties Metric Imperial
Density 7.94 g/cm³ 0.287 lb/in³
Melting point 1357-1385 °C 2475-2525 °F

Mechanical properties of Incoloy UNS N08811 pipe

Properties Metric Imperial
Tensile strength (annealed) 560 MPa 81200 psi
Yield strength (annealed) 250 MPa 36300 psi
Elongation at break (annealed prior to test) 45% 45%

 

Incoloy Alloy UNS N08811 pipeIncoloy Alloy UNS N08811 pipeIncoloy Alloy UNS N08811 pipe

Hot Tags: incoloy alloy uns n08811 pipe, China incoloy alloy uns n08811 pipe suppliers, alloy for semiconductors, precision alloy rod, alloy for dies, corrosion resistant material, alloy for digital manufacturing baths, alloy products