INCOLOY® alloy 020 (UNS N08020) has excellent corrosion resistance in chemical environments containing sulfuric acid, and useful resistance to environments containing chlorides, nitric acid, and phosphoric acid. Other uses include the production of gasoline, solvents, explosives, inorganic and organic chemicals, pharmaceuticals, and food and synthetic materials. INCOLOY alloy 020 is readily fabricated to produce mixing tanks, heat exchangers, process piping, pickling equipment, pumps, valves, fasteners and fittings. Applications for alloy 020 requiring resistance to aqueous corrosion are essentially the same as those for INCOLOY alloy 825.
Main Standards
ASTM B729
Seamless Pipe & Tube
ASTM B829
Seamless Pipe & Tube
ASTM B464
Welded Pipe
ASTM B775
Welded Pipe
ASTM B468
Welded Tube
ASTM B751
Welded Tube
ASTM B751
Electric Fusion Welded Pipe
ASTM B366
Welded Fittings
ASTM B462
Flange and Forged Fittings
ASTM B472
Billets and Bars
ASTM B473
Bar and Wire
ASTM B475
Round Weaving Wire
ASTM B463
Plate, Sheet and Strip
ASTM B906
Plate, Sheet and Strip
ASTM A240
Plate, Sheet and Strip
ASTM A480
Plate, Sheet and Strip
Chemical Composition
Data Sheet
Physical Properties
| Density | g/cm3 | 8.08 | |
|---|---|---|---|
| lb/in.3 | 0.292 | ||
| Specific Heat | Btu/lb-°F | 0.12 | |
| J/kg-°C | 500 | ||
| Thermal Conductivity at 200°F (93°C) | Btu-in/ft2-h-°F | 85 | |
| W/m-°C | 12.3 | ||
| Electrical Resistivity | ohm circ mil/ft | 651 | |
| μΩ-m | 1.08 | ||
| Young's Modulus (70°F) | 103 ksi | 28 | |
| GPa | 193 | ||
| Shear Modulus (70°F) | 103 ksi | 11 | |
| GPa | 76 | ||
| Coefficient of Expansion | 77-212°F, 10-6 in/in•°F | 8.2 | |
| 25-100°C, μm/m•°C | 14.7 | ||
Mechanical Properties
| Tensile Strength | ksi | 90 |
|---|---|---|
| MPa | 620 | |
| Yield Strength (0.2% Offset) | ksi | 45 |
| MPa | 300 | |
| Elongation | % | 40 |




FAQ
Q: How do you control quality ?
A: Mill Test Certification is supplied with shipment, Third Party Inspection is available. and we also get ISO,SGS,Alibaba Verified.
Q: What are the advantages of your company ?
A: We have many professionals, technical personnel, more competitive prices and best after-dales service than other stainless steel companies.
Q: How many coutries you already exported ?
A: Exported to more than 50 countries mainly from America, UK, Kuwait, Egypt, Turkey, Jordan,India, etc.
Q: Can you provide sample ?
A: Yes. We can provide the small samples in stock for free, as long as you contact us.Customized samples will take about 5-7 days.
Hot Tags: incoloy 020, China incoloy 020 suppliers, alloy for aging, alloy for heating baths, alloy for refurbishment baths, incoloy seamless pipe, alloy for actuators, alloy for dentistry baths
Previous
Incoloy 028Next
Incoloy 945XYou Might Also Like
Send Inquiry