C4 G30 Thick wall Hastelloy Alloy Tube
video

C4 G30 Thick wall Hastelloy Alloy Tube

Specifications
Plate, Sheet and Strip: ASTM B582, ASME SB582
Bar and Rod: ASTM B581, ASME SB581
Seamless Pipe: ASTM B622, ASME SB622
Welded Pipe: ASTM B619/B626, ASME SB619/SB626
Fittings: ASTM B366/B462, ASME SB366/SB462
Forgings: ASTM B462, ASME SB462
Others: NACE MR0175, ISO 15156
Send Inquiry
Chat Now

As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.

Product Introduction

Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of c4 g30 thick wall hastelloy alloy tube in China. If you're going to wholesale high quality c4 g30 thick wall hastelloy alloy tube made in China, welcome to get free sample from our factory. Good service and reasonable price are available.

 

Hastelloy Pipe Products Application

C4 G30 seamless tube video

 

Hastelloy G30 Tube Specifications

Size 15 NB to 150 NB IN
Type Seamless / ERW / Welded / Fabricated / Hollow / LSAW Pipes
wall thickness 035" –.095′, (special wall thicknesses available)
Schedule SCH5, SCH10, SCH40, STD, SCH80, SCH160
Finish Polished, AP (Annealed & Pickled), BA (Bright & Annealed), MF
Form Round, Square, Rectangular, Hydraulic, Straight or 'U' bent Tubes Etc
Length Single Random, Double Random & Cut Length.
End Plain End, Beveled End, Treaded.
Hastelloy C4 Pipe and Tube Specification

SPECIFICATIONS : ASTM B622, B619, B626 / ASME SB622, SB619, SB626
STANDARD : ASTM, ASME and API
SIZE RANGE : 15"NB – 150"NB
OUTER DIAMETER : 1.250″ – 6.000″ (30-150mm)
WALL RANGE : 0.095″ – 1.000″ (.2.5-25mm)
SCHEDULE : SCH 10, SCH20, SCH30, SCH40, STD, SCH60, XS, SCH80, SCH120, SCH140, SCH160, XXS
TYPE : Seamless / ERW / Welded / Fabricated / LSAW Pipes
LENGTH : Single Random, Double Random & Cut Length
FORM : Round Pipes/Tubes, Square Pipes/Tubes, Rectangular Pipe/Tubes, Coiled Tubes, "U" Shape, Pan Cake Coils, Hydraulic Tube

 

Hastelloy Material Specification

Hastelloy G-30 Tube Chemical Composition

Element Content (%)
Nickel, Ni 43
Chromium, Cr 28.0-31.5
Iron, Fe 13-17
Cobalt, Co 5
Molybdenum, Mo 4-6
Tungsten, W 1.50 – 4
Manganese, Mn 1.50
Copper, Cu 1 – 2 .40
Silicon, Si 0.8
Phosphorous, P 0.040
Carbon, C 0.030
Sulfur, S 0.020
C4 – UNS N06455
Element Simbol Maximum
Carbon C 0,015
Manganese Mn 1,0
Titanium Ti 0,70
Sulfur S 0,030
Silicon Si 0,08
Nickel Ni Balance
Chrome Cr 14,0-18,0
Molybdenum Mo 14,0-17,0
Cobalt Co 2,0
Phosphorus P 0,04
Iron Fe 3,0

C4 G30 Alloy tube

C4 G30 stainless steel tube suppliersC4 G30 seamless Alloy tube price

Hastelloy C4Hastelloy C4 alloy is an austenitic low carbon nickel-molybdenum-chromium alloy. The main difference from other alloys of similar chemical composition developed earlier is the low carbon, silicon, iron, tungsten content and the addition of stabilizing elements titanium. Such a chemical composition is more suitable for manufacturing corrosion-resistant equipment that requires welding, and also has good cold and hot plasticity.
Hastelloy G-30 alloy has excellent corrosion resistance and high temperature strength, and can work stably for a long time in harsh environments of high temperature and pressure. Its corrosion resistance is better than other nickel-based alloys, especially in oxidizing media and acidic environments. In addition, Hastelloy G-30 also has excellent processing performance and welding performance, and can meet the requirements of various complex manufacturing processes.

Products Description

C4 G30 Thick wall Alloy Tube

C4 G30 Thick wall Hastelloy Alloy Tube

Customer Case

customer visit

C4 G30 hastelloy piping dealer

C4 G30 ss steel tubing factory

AQ

Q: Can you send samples?
A: Of course, we can send samples to all over the world, our samples are free, but customers need to bear the express cost.

Q: What shipping ports are there?
A: Generally, we ship from Tianjin Port, you can choose other ports according to your needs.

Q: About the product price?
Answer: Due to cyclical changes in raw material prices, prices vary in different periods.

Q: About the product price of C4 G30 Alloy tube?
A: Due to cyclical changes in raw material prices, prices vary in different periods.

Contact Us

 

Address

No.4-1114 Beichen Building, Beicang Town, Beicheng District, Tianjin City, China

 

Phone

+86-15824687445

 

Email

ss@gneesteel.com

 

Skype

mmkelly1314

 

Whatsapp/Wechat

+86 15824687445

 

Hot Tags: C4 G30 Thick wall Hastelloy Alloy Tube, China C4 G30 Thick wall Hastelloy Alloy Tube suppliers, alloy for tempering, alloy for scrubbers, alloy for grinding, stainless steel pipe, Hastelloy B, nickel chromium molybdenum alloy

Send Inquiry

whatsapp

Phone

E-mail

Inquiry