Hastelloy C4
video

Hastelloy C4

C: 0.015 max
Mn: 1.0 max
Si: 0.08 max
P: 0.040 max
S: 0.030 max
Cr: 14.0 – 18.0
Ci: 2.0 max
Mo: 14.0 – 17.0
Ti: 0.70 max
Fe: 3.0 max
Ni: Balance
Send Inquiry
Chat Now

As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.

Product Introduction

Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of hastelloy c4 in China. If you're going to wholesale high quality hastelloy c4 made in China, welcome to get free sample from our factory. Good service and reasonable price are available.

 

Hastelloy C4 is a nickel-chromium-molybdenum alloy which has improved thermal stability. In this alloy, the tungsten was totally omitted and the iron content was reduced to approximately 1%. The alloy also contains approximately 0.3% Ti.

Outstanding high-temperature stability; exhibits good ductility and corrosion resistance after long-time aging at 650 to 1040 °C (1200–1900 °F). Resists formation of grain-boundary precipitates in weld heat-affected zones, and is suitable for most chemical process applications in the as-welded condition. Has excellent resistance to stress-corrosion cracking and to oxidizing atmospheres up to 1040 °C (1900 °F).

Hastelloy C4 has exceptional resistance to a variety of chemical process environments, including hot contaminated mineral acids, solvents, chlorine, and chlorine-contaminated media (organic and inorganic, dry chlorine, formic and acetic acids, acetic anhydride, seawater, and brine). The general corrosion resistance of Alloy C276 and Alloy C4 was essentially the same in many corrosive environments, except that in strongly reducing media like hydrochloric acid, Alloy C276 was better; but in highly oxidizing media, the opposite was true, that is, Alloy C4 was better. Alloy C4 offers good corrosion resistance to a wide variety of media including organic acids and acid chloride solutions. This alloy has found greater acceptance in European countries in contrast to Alloy C276, which is more widely used and accepted in the United States.

 

Product Parameter
 

 

Element

Min %

Max %

Cr

14.00

18.00

Mo

14.00

17.00

Fe

–

3.00

C

–

0.015

Si

–

0.08

Co

–

2.00

Mn

–

1.00

P

–

0.04

S

–

0.03

Ti

–

0.70

 

Application
 

 

Environmental engineering: wastewater treatment, e.g. evaporation plants and crystallizers o Construction components in waste incineration plants and flue gas desulfurization plants, e.g. piping, dampers, absorbers, blowers, agitators and heat exchangers o Chemical engineering, e.g. heat exchangers, piping, fittings, measurement probes and centrifuges o Plant equipment for de-acidifiers, e.g. vessels, piping, heat exchangers, gate valves and dampers o Storage and transport vessels for acids.

 

Features
 

 

HASTELLOY C-4 alloy (UNS N06455) is the most (microstructurally) stable of the widely used nickel-chromium-molybdenum materials, which are well known for their resistance to many aggressive chemicals, in particular hydrochloric acid, sulfuric acid, and chlorides. This stability means that the alloy can be welded without fear of sensitization, i.e. the nucleation and growth of deleterious, second phase precipitates in the grain boundaries of the weld heat-affected zone (HAZ).

 

Like other nickel alloys, it is ductile, easy to form and weld, and possesses exceptional resistance to stress corrosion cracking in chloride-bearing solutions (a form of degradation to which the austenitic stainless steels are prone). With its high chromium and molybdenum contents, it is able to withstand both oxidizing and non-oxidizing acids, and is resistant to pitting and crevice attack in the presence of chlorides and other halides.

 

Our Company
 

 

product-750-750

38000㎡ workshop and 200+ emplovees to meet your huge demands.

 

Packing & Delivery
 

 

product-750-750

 

Customer Visit
 

 

product-750-750

Gnee exports steel to over 70 countries and collaborates with more than 600 companies worldwide

 

FAQ
 

 

Q: Are you a factory or trading company?

A: We are professional manufacturer, and our company also is a very professional a trade company for steel products.We can provide a wide range of steel products.

Q:What do your factory do regarding quality control?

A: We have obtained ISO, CE and other certifications. From materials to products, we check every process to maintain good quality.

Q: Can I get samples before order ?

A: Yes, of course. Usually our samples are free. we can produce by your samples or technical drawings.

 

Hot Tags: hastelloy c4, China hastelloy c4 suppliers, alloy for fuel cells, UNS N06455 N10629 Hastelloy Pipe, alloy for petrochemical applications, alloy for piping systems, alloy for annealing, hastelloy ss piping

Send Inquiry

whatsapp

Phone

E-mail

Inquiry