UNS N06002 N10665 N06455 Hastelloy Steel Pipe
As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.
- Send E-mail: ss@gneesteel.com
Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of uns n06002 n10665 n06455 hastelloy steel pipe in China. If you're going to wholesale high quality uns n06002 n10665 n06455 hastelloy steel pipe made in China, welcome to get free sample from our factory. Good service and reasonable price are available.
Product Description
UNS N06002 N10665 N06455 hastelloy steel tube video
Excellent oxidation resistance at high temperature(>1200℃)).
Good high-temperature strength.
Good formability and weldability.
Good resistance to stress corrosion cracking.
Product Specification
| Nominal Composition (Weight%) | |
|---|---|
| Ni | 47 Bal. |
| Cr | 22 |
| Fe | 18 |
| Mo | 9 |
| Co | 1.5 |
| W | 0.6 |
| C | 0.1 |
| Mn | 1 Max. |
| Si | 1 Max. |
| B | 0.008 Max. |
| Nb | 0.5 Max. |
| Al | 0.5 Max. |
| Ti | 0.15 Max. |
UNS N06002 N10665 N06455 hastelloy steel tubing


Alloy X (N06002, 2.4665) alloy can be easily processed hot and cold and machined using ordinary processes. However, due to the high strength of the material, high-power equipment is required for hot and cold processing. Alloy X (N0600, 2.4665) alloy has excellent weldability and can be welded with any convenient welding process.
Nickel-molybdenum alloy Hastelloy B-2 has extremely low carbon and silicon content, which reduces the precipitation of carbon and other impurity phases in the welding heat-affected zone, so its welds also have sufficient corrosion resistance.
n06455 nickel-based high-temperature alloy is mainly composed of nickel, chromium, cobalt, molybdenum, aluminum, titanium and other elements. Nickel is the main component of the alloy and can improve the corrosion resistance and oxidation resistance of the alloy.
Customer Case
GNEE customer visit


FAQ
Q: How many countries have you exported to?
A: Exported to more than 50 countries, mainly from the United States, Russia, the United Kingdom, Kuwait, Egypt, Turkey, Jordan, India, etc.
Q: Can you provide samples?
Answer: Yes. As long as you contact us, we can provide free small samples in stock. Customized samples will take about 5-7 days.
Q: Can you send samples?
A: Of course, we can send samples to all over the world, our samples are free, but customers need to bear the express cost.
Q: About the product price of UNS N06002 N10665 N06455 hastelloy steel tubing?
A: Due to cyclical changes in raw material prices, prices vary in different periods.
Contact Us
One-stop service, making choices easier.
![]()
Phone
+8615824687445
+86-372-5055135
![]()
ss@gneesteel.com
![]()
Address
No.4-1114, Beichen Building, Beicang Town, Beichen District, Tianjin, China
Hot Tags: uns n06002 n10665 n06455 hastelloy steel pipe, China uns n06002 n10665 n06455 hastelloy steel pipe suppliers, alloy for scrubbers, hastelloy ss pipe, alloy for industrial equipment, alloy for petrochemical applications, hastelloy material piping alloy, piping seamless stainless steel
You Might Also Like
Send Inquiry