Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of hastelloy n s w seamless pipe in China. If you're going to wholesale high quality hastelloy n s w seamless pipe made in China, welcome to get free sample from our factory. Good service and reasonable price are available.

 

Hastelloy N S W Seamless Pipe Equivalent grade

Hastelloy N S W seamless pipes video

GNEE STEEL GROUP supplies Hastelloy N S W Seamless Pipe for you

 

GNEE STEEL GROUP supplies Hastelloy N Seamless Pipe

Available forms of Hastelloy N
– Round bars, wire rods, forgings
– Sheets, boards
– Seamless pipes, welded pipes
– Fittings and flanges
– Non-standard customized parts

Hastelloy N product forms and standards:

● Bars, wires and forgings: ASTM B573, ASME SB573, AMS 5771

● Plate, sheet and strip: AMS 5607, ASTM B434, ASME SB434

● Welding products: ERNiMo-2 A5.14

● Others: ASTM B366, ASME SB366

GNEE STEEL GROUP supplies Hastelloy S Seamless Pipe

Equivalent name: UNS N06635
Specification:
Wire: 0.04-10mm
Strip: 0.05-15mm*3-600mm
Rod: 3mm~800mm;
Pipe: outer diameter 1-1000 mm; thickness 0.1-100 mm
Plate: thickness 0.15-180mm; width 8-3000mm; length 500mm-11000mm
Surface finish: black, bright polished, rough turned, No 4 finish, matte finish, bA finish or other finishing.

GNEE STEEL GROUP supplies Hastelloy W Seamless Pipe

Standards : AMS 5755, AMS 5786, AWS A5.14 & ASME SFA 5.14
Dimensions : EN, DIN, JIS, ASTM, BS, ASME, AISI
Wire : Thickness starting from 0.05mm
Round bar size : Diameter: 3-~800mm
Hex Bar size : 2-100mm A/F
Flat bar size : Thickness: 2 -100mm / Width: 10 to 500mm
Square bar size : 4 to 100mm
Rectangular Bars Size : 33 x 30mm to 295 x 1066mm
Hollow Bar : 32mm OD x 16mm ID to 250mm OD x 200mm ID
Tolerance : H8, H9, H10, H11, H12, H13K9, K10, K11, K12 or as per clients' requirements
Finish : Black, Bright Polished, Rough Turned, NO.4 Finish, Matt Finish, BA Finish

 

Hastelloy N S W Seamless Pipe chemical composition

 Hastelloy N Seamless Pipe chemical composition

Grade C Mn Si Cu Ni Cr Mo W Fe
Hastelloy N 0.06 max 0.8 max 1.00 max ≤ 0.35 71 Balance 6.0 – 8.0 15.0 – 18.0 ≤ 0.50 ≤ 5

Hastelloy S Seamless Pipe chemical composition

Elements Content (%)
Nickel, Ni 67
Chromium, Cr 14.5 - 17
Molybdenum, Mo 14 - 16.5
Iron, Fe 3
Cobalt, Co 2
Tungsten, W 1
Copper, Cu 0.35
Manganese, Mn 0.30 - 1.0
Silicon, Si 0.20 - 0.75
Aluminum, Al 0.10 - 0.50
Carbon, C 0.020
Phosphorous, P 0.020
Boron, B 0.015
Sulfur, S 0.015
Lanthanum, La 0.010 - 0.10

Hastelloy W Seamless Pipe chemical composition

The Chemical Composition of Hastelloy W, %
Ni Balance≤63.0
Cr ≤5.0
Fe ≤6.0
Co ≤2.5
Mo ≤24.0
C ≤0.12
Mn ≤1.0
Si ≤1.0

Hastelloy N S W alloy seamless pipe

Hastelloy N S W seamless tube suppliersHastelloy N S W metal seamless pipe price

Hastelloy N alloy is a nickel-based high-temperature alloy material used in molten salt reactors. It has excellent corrosion resistance, resistance to neutron radiation and good high-temperature mechanical properties. 
Hastelloy S (also known as Alloy S), designated UNS N06635, is a nickel-based alloy with excellent thermal stability, low thermal expansion and oxidation resistance at 1095 °C [2000 °F]. Retains strength and ductility after aging at 425 to 870 °C [800 to 1600 °F].

Hastelloy W alloy is a nickel-based alloy composed of nickel, molybdenum, chromium, cobalt and other elements. Hastelloy W alloy has a nickel content of approximately 60%. Hastelloy W is a solid solution strengthened alloy, mainly used for welding dissimilar alloys.

 

Hastelloy N S W Seamless Pipe material & size

Hastelloy N S W Seamless Pipe material & size

Hastelloy N S W Seamless Pipe

Hastelloy N S W Seamless Pipe

 

Customer Case

GNEE customer visit

Hastelloy N S W Seamless Pipe

 

FAQ

Q: How many countries have you exported to?
A: Exported to more than 50 countries, mainly from the United States, the United Kingdom, Kuwait, Egypt, Turkey, Jordan, India, etc.

Q: Can I get your best price?
A: Our goal is to provide you with the best price and excellent quality assurance in the long run. Please leave your contact information to get the best quote, we will provide you with the best solution as soon as possible.

Q: How long is your delivery time?
A: Generally it is 5-10 days if the goods are in stock. Or if the goods are not in stock, it is 15-20 days, depending on the quantity.

Q: About the product price of Hastelloy N S W seamless pipe?
A: Due to cyclical changes in raw material prices, prices vary in different periods.

Contact Us

One-stop service, making choices easier.

icon1

Phone

+8615824687445

+86-372-5055135

icon2

Email

ss@gneesteel.com

icon3

Address

No.4-1114, Beichen Building, Beicang Town, Beichen District, Tianjin, China

 

Hot Tags: hastelloy n s w seamless pipe, China hastelloy n s w seamless pipe suppliers, alloy for coating, alloy for grinding, alloy for pumps, nickel chromium iron alloy, material piping, UNS N06455 N10629 Hastelloy Pipe

You Might Also Like

Send Inquiry

whatsapp

Phone

E-mail

Inquiry