Incoloy 800 Buttweld Fittings
As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.
- Send E-mail: ss@gneesteel.com
Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of incoloy 800 buttweld fittings in China. If you're going to wholesale high quality incoloy 800 buttweld fittings made in China, welcome to get free sample from our factory. Good service and reasonable price are available.
Incoloy 800 Buttweld Fittings
Product Introduction
Incoloy 800 buttweld fittings are components used in piping systems to connect, control, and change the direction of the flow of liquids or gases. These fittings are manufactured using Incoloy 800 alloy, which imparts its high-temperature corrosion resistance properties to the fittings. The buttweld construction involves welding the fittings to the pipes, creating a strong and leak-resistant joint.
INCONEL 800H BUTTWELD FITTINGS SIZE & SPECIFICATION
| Specification | ASTM B366 / ASME SB366 |
| Standard | EN, ISO, DIN, JIS, NPT |
| Dimension Standard | ASME/ANSI B16.9, ASME B16.28, MSS-SP-43 |
| Thickness | SCH10, SCH20, SCH30, STD SCH40, SCH60, XS, SCH 80, SCH 100, SCH 120, SCH 140, SCH 160, XXS available with NACE MR 01-75 |
| Size | 1/8" NB TO 48" NB. (Seamless & 100% X-Ray Welded, Fabricated) |
| Bending Radius | R=1D, 2D, 3D, 5D, 6D, 8D, 10D or Custom ASTM A403 Grade WP317L Pipe Fitting |
| Type | Seamless / Welded / Fabricated |
| Pressure-Temperature Class | 150LB, 300LB, 600LB, 1500LB, 2500LB. |
| Schedule | Schedule 5 TO Schedule XXS. |
| Type Of Dimension | BS1640, EN 10253 - 4, DIN 2605, JIS B2312, ANSI B16.9, MSS SP-75, ANSI B16.28, MSS-SP-43 Type A, MSS-SP-43 Type B, JIS B2313 |
Characteristics and advantages of Incoloy 800 buttweld fittings include:
High-Temperature Resistance: Incoloy 800 fittings are designed to withstand temperatures up to 1100°C (2010°F) in oxidizing atmospheres and up to 816°C (1500°F) in reducing environments. This makes them suitable for applications in heat exchangers, furnaces, and other high-temperature processing equipment.
Corrosion Resistance: These fittings offer excellent resistance to corrosion, both in oxidizing and reducing environments, making them ideal for use in chemical processing plants and other industries where corrosion is a concern.
Oxidation Resistance: Incoloy 800 fittings have a protective oxide layer that forms on the surface at high temperatures, providing resistance to oxidation and scaling, even in atmospheres containing sulfur compounds.
Strength and Ductility: The alloy's combination of nickel, iron, and chromium provides a balance of mechanical properties, including good strength and ductility, allowing the fittings to maintain their integrity under stress.
Weldability: Incoloy 800 buttweld fittings are easily weldable using common welding methods, allowing for secure connections between components.
Versatility: These fittings can be used in a wide range of applications, including heat exchangers, furnace components, petrochemical processing, power generation, and more.
Hot Tags: incoloy 800 buttweld fittings, China incoloy 800 buttweld fittings suppliers, engineering alloy, oxidation resistant alloy, Monel K500 Nickel Alloy Pipe, construction alloy, heat resistant alloy, durable alloy