Gh4169 Oxidation resistant alloy Plate
video

Gh4169 Oxidation resistant alloy Plate

Nickel + Cobalt: 50.00 -55.00
Chromium: 17.00-21.00
Molybdenum: 2.80 -3.30
Columbium + Tantalum: 4.75 -5.50
Titanium: 0.65 -1.15 Aluminum: 0.20 -0.80
Cobalt: 1.00 max Carbon: 0.80 max
Manganese: 0.35 max Silicon: 0.35 max
Phosphorus: 0.015 max Sulfur: 0.015 max
Boron: 0.006 max Copper: 0.30 max
Iron: Balance
Send Inquiry
Chat Now

As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.

Product Introduction

Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of gh4169 oxidation resistant alloy plate in China. If you're going to wholesale high quality gh4169 oxidation resistant alloy plate made in China, welcome to get free sample from our factory. Good service and reasonable price are available.

 

Gh4169 Oxidation resistant alloy Plate introduce

Gh4169 Oxidation resistant alloy Plate

Gh4169 Oxidation resistant alloy PlateGh4169 Oxidation resistant alloy Plate

GH4169 alloy is a nickel-based high-temperature alloy precipitated and strengthened by body-centered square γ" and face-centered cubic γ' phases. It has good comprehensive properties in the temperature range of -253~700℃, and the yield strength below 650℃ ranks among the highest deformation temperatures. It ranks first among alloys and has good fatigue resistance, radiation resistance, oxidation resistance, corrosion resistance, as well as good processing performance, welding performance and long-term structural stability. It can manufacture various parts with complex shapes and is used in aerospace, nuclear energy, In the petroleum industry, it has been widely used in the above temperature range.

GH4169 nickel-based alloy plate, with its unique chemical composition and phase composition, exhibits excellent high temperature strength, corrosion resistance and processing performance, and is widely used in high-end industrial fields such as aerospace, nuclear energy, and petrochemicals. In practical applications, through precise heat treatment and processing technology, its performance potential can be further exerted to meet various stringent application requirements.

GH4169 alloy Production Forms

Product Condition
Sheet hot or cold rolled, bright/solution annealed, pickled or de-scaled
Strip cold rolled, bright/solution annealed, pickled or de-scaled
Pipe longitudinally welded or seamless, solution annealed, pickled or de-scaled
Bar hot rolled or forged, solution annealed, pickled or de-scaled
Wire rolled or drawn, solution annealed, pickled or de-scaled
Forging solution annealed, machined on request
Welding filler metal welding bar, wire electrode, coated bar electrode

Gnee Steel customer visit

Gh4169 Plate

Gh4169 Oxidation resistant alloy Plate

GNEE Group Factory Environment

Gh4169 Oxidation resistant Plate

Gh4169 Oxidation resistant alloy Plate

GNEE Group Product Packaging

Gh4169 alloy Plate

Gh4169 Oxidation resistant alloy Plate

FAQ
Q. How do you control quality ?
A: Mill Test Certification is supplied with shipment, Third Party Inspection is available. and we also get ISO,SGS Verified.
Q: What are the advantages of your company ?
A: We have many professionals, technical personnel, more competitive prices and best after-dales service than other stainless steel companies.
Q: How many coutries you already exported ?
A: Exported to more than 50 countries mainly from America, UK, Kuwait, Egypt, Turkey, Jordan,India, etc.

Hot Tags: Gh4169 Oxidation resistant alloy Plate, China Gh4169 Oxidation resistant alloy Plate suppliers, Monel 400 Alloy Steel Sheet, Cold Rolled Inconel 625 Alloy Seamless Pipe, Hastelloy C276 ROUND BAR, Alloy Steel 600 plate, Ni36CrTiAl Plate, 2 4668 Nickel Alloy Steel Coil