GH3536 3230 High Temperature Nickel Alloys Pipe
As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.
- Send E-mail: ss@gneesteel.com
Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of gh3536 3230 high temperature nickel alloys pipe in China. If you're going to wholesale high quality gh3536 3230 high temperature nickel alloys pipe made in China, welcome to get free sample from our factory. Good service and reasonable price are available.
GH3536 3230 High Temperature Nickel Alloys Pipe Products Description
GH3536 3230 high temperature steel Pipe video
GNEE STEEL GROUP supplies GH3536 GH3230 High Temperature Nickel Alloys Pipe for you
GH3536 High Temperature Nickel Alloys Pipe
Density:8.44 g/c㎡
Melting range:1290-1350℃
Size: OD 25~320mm
W.T: 0.5 - 100mm
Length: 5.8m, 6m, 11.8m, 12m
Type: Seamless/welded
Standards:
Seamless Pipe / Tube: ASTM B444, ASTM B829, AMS 5581
Welded Pipe/tube: ASTM B705, ASTM B775, ASTM B704, ASTM B751
|
Product Name |
GH3230 High Temperature Nickel Alloys Pipe |
|
Length |
1m~12m or as required |
|
Outside Diameter |
8mm-426mm (3/8"-100") or as required |
|
Wall Thickness |
0.1mm-6mm (SGH10-XXS) or as required |
|
Standard |
AISI.ASTM.DIN.JIS.GB.SUS.EN.etc |
GH3536 3230 High Temperature Nickel Alloys Pipe Professional Customization
| Cold-drawn Wire | ¢0.3~¢18mm(Delivery in rolls or trays) |
| Hot-Rolling Wire | ¢5.5~¢20mm(Delivery in rolls) |
| Strip | thickness 0.1~4.5*width 6~350mm(Supply in rolls or straight strips) |
| Smooth Forged Rod on a Lathe |
¢60~350mm,L800-2500mm |
| Hot-rolled Burnishing | ¢20~80mm,L1000-5000mm |
| Cold Drawn and Burnishing | ¢2.5~18mm,L1000-8000mm |
| Seamless Tube | ¢1~275mm,wall thickness 0.2~30,L1000-8000mm |
GH3536 3230 High Temperature Nickel Alloys Pipe chemical composition
GH3536 High Temperature Nickel Alloys Pipe chemical composition
| Ni | Cr | Fe | C | Mn | Si | Mo | Co | Al | W | B | P | S | |
| Min | 20.5 | 17.0 | 0.05 | 8.0 | 0.5 | 0.2 | |||||||
| Max | Rem | 23.5 | 20.0 | 0.15 | 1.0 | 1.0 | 10.0 | 2.5 | 0.1 | 1.0 | 0.005 | 0.015 | 0.01 |
GH3230 High Temperature Nickel Alloys Pipe chemical composition
| C | Cr | W | Mo | Mn | Al | Ti | Co |
| 0.093 | 21.56 | 14.62 | 1.32 | 0.51 | 0.33 | 0.05 | 1.49 |
| Si | La | B | Fe | S | P | Ni | |
| 0.41 | 0.015 | 0.005 | 0.51 | 0.001 | 0.011 | Bal. | |
GH3536 3230 high temperature nickel alloys Pipe


GH3536 alloy is a nickel-based high-temperature alloy mainly solid-solution strengthened with chromium and molybdenum (the corresponding brand is Hastelloy-X). It has good oxidation resistance and corrosion resistance, and still has moderate durability and creep strength at 900°C. , suitable for manufacturing hot-end components of high-temperature service structures, such as tail cones, vortex exhaust pipes, and combustion nozzle housings.
GH3230 superalloy is a nickel-based deformed superalloy with an extremely high degree of alloying, including a total content of up to 36% W+Mo+Cr. This alloy strengthens the matrix through solid solution alloy elements. The addition of W and Mo not only improves the creep resistance, but also increases the stacking fault energy, thereby inhibiting the occurrence of dislocation slip.
Product technology


Customer Case
customer visit

FAQ
Q: Can you provide us samples, is it free or does it require payment?
A: If you don't need to print your logo or other artwork on the product, we won't charge any fee, just tell us your freight collect account, such as Fedex, DHL, TNT. If you don't have it, we need to charge the express fee appropriately.
Q: Can I get your best price?
A: Our goal is to provide you with the best price and excellent quality assurance in the long run. Please leave your contact information to get the best quote, we will provide you with the best solution as soon as possible.
Q: About the product price of GH3536 3230 high temperature nickel alloys Pipe?
A: Due to cyclical changes in raw material prices, prices vary in different periods.
Contact Us
Address
No.4-1114 Beichen Building, Beicang Town, Beicheng District, Tianjin City, China
Phone
+86-15824687445
ss@gneesteel.com
Skype
mmkelly1314
Whatsapp/Wechat
+86 15824687445
Hot Tags: gh3536 3230 high temperature nickel alloys pipe, China gh3536 3230 high temperature nickel alloys pipe suppliers, Casting High Temperature Alloy
You Might Also Like
Send Inquiry