1.4005 416 Stainless Steel Peeled Round Bar
video

1.4005 416 Stainless Steel Peeled Round Bar

SS 1.4005 bar has lower corrosion resistance than other common austenitic stainless steel grades. It is resistant to dry atmospheres, fresh water and milk acids and alkalies but less so than its equivalent non-free-machining grades. It is less corrosion resistant than 17% chromium ferritic alloys such as grade 430. The high sulphur content in 1.4005 stainless steel makes it unsuitable for use in marine environments or environments exposed to chloride. Max corrosion resistance can be achieved in the hardened condition with a smooth surface finish.
Send Inquiry
Chat Now

As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.

Product Introduction

Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of 1.4005 416 stainless steel peeled round bar in China. If you're going to wholesale high quality 1.4005 416 stainless steel peeled round bar made in China, welcome to get free sample from our factory. Good service and reasonable price are available.

 


1.4005 Stainless Steel Rod is a martensitic machining bar with machinability enhanced through the addition of phosphorus and sulphur.It has the highest machinability of any stainless steel, at about 85% of that of a free-machining carbon steel. As for most other free-machining stainless steels the improvement in machinability is achieved by addition of sulphur which forms manganese sulphide inclusions; this sulphur addition also lowers the corrosion resistance, weldability and formability to below that of its non-free machining equivalent grade 410.

304l-stainless-steel-round-bar

ss peal bar

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

The Chemical Element Of 1.4005 Stainless Steel Bar

EN 10088-3

Chemical Element % Present

Carbon (C)

0.06 - 0.15

Chromium (Cr)

12.00 - 14.00

Manganese (Mn)

0.00 - 1.50

Silicon (Si)

0.00 - 1.00

Phosphorous (P)

0.00 - 0.04

Sulphur (S)

0.15 - 0.35

Molybdenum (Mo)

0.00 - 0.60

Iron (Fe)

Balance

 

Bar Up to 160mm Dia or Thickness

EN 10088-3

Mechanical Property Value

Proof Stress

450 Min MPa

Tensile Strength

650 - 850 MPa

 

Grade 416/1.4005 has the best machinability of all stainless steel grades, around 85% of that of a free machining carbon steel. This improved machinability is achieved by the addition of sulphur in the chemical composition. This forms manganese sulphide inclusions, and this addition of sulphur also reduces the corrosion resistance, weldability and formability to lower than that of its non-free machining equivalent, 410.

 

Customer Visit 

GNEE Steel Group is China's professional one-stop supply chain enterprise for steel products. Its stainless steel pipe production technology has reached the world's average technical level. It has been recognized by dozens of project companies and has become a star enterprise in Asia.

 

gnee steel

Hot Tags: 1.4005 416 stainless steel peeled round bar, China 1.4005 416 stainless steel peeled round bar suppliers, 420 Stainless H type Steel, Stainless Steel 446 Round Bar, Stainless Steel 310S Round Bar, 304 316 Steel Flat Bars With Holes, 304 304L 316 316L Stainless Round Bar

Send Inquiry

whatsapp

Phone

E-mail

Inquiry