431 Stainless Round Bar
As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.
- Send E-mail: ss@gneesteel.com
Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of 431 stainless round bar in China. If you're going to wholesale high quality 431 stainless round bar made in China, welcome to get free sample from our factory. Good service and reasonable price are available.
PRODUCT INTRODUCTION
431 is a high chromium-low nickel high hardenability Martensitic stainless steel with high strength and good corrosion resistance, as generally supplied hardened and tempered in the tensile range 850 - 1000 Mpa (condition T) Brinell range 248 - 302.


Characterised by very good corrosion resistance in general atmospheric corrosive environments, good resistance to mild marine and industrial atmospheres, resistant to many organic materials, nitric acid and petroleum products coupled with high tensile and high yield strength plus excellent toughness in the hardened and tempered condition. 431 due to its excellent hardenability is capable of being through hardened up to Rc44, depending upon carbon content and section size. Small sections can be air cooled and larger sections oil quenched for maximum through hardness.Pre hardened and tempered 431 will also respond readily to nitriding achieving a typical surface hardness of over Rc65. The nitriding process however reduces the corrosion resistance and is therefore not generally recommended except for critical applications where the benefit outweighs all other considerations.
Used extensively for parts requiring a combination of high tensile strength, good toughness and good corrosion resistant properties.
Typical applications are: Aircraft Parts and Components, Bolts and Nuts, Fasteners, Pump Shafts, Propellor Shafts, Studs, Valve Parts etc.
Material magnetic in all conditions.
FAQ
Q: Can we visit your factory?
A: Warmly welcome. Once we have your schedule, we will arrange the professional sales team to follow up your case.
Q: Can you provide sample?
A: Yes, for regular sizes sample is free but buyer need to pay freight cost.
Q:How can I get a quotation from you?
A:You can leave us message, and we will reply every message in time. Or we may talk on line by trade manager. And you can also find our contact information on contact page.
Q: How could you guarantee your products?
A: Each piece of products is manufactured by certified workshops, inspected by piece by piece according to national QA/QC standard. We also could issue the warranty to customer to guarantee the quality.
Hot Tags: 431 stainless round bar, China 431 stainless round bar suppliers, 420 Stainless H type Steel, 304 304L 316 316L Stainless Round Bar, 304 316 Steel Flat Bars With Holes, Stainless Steel 446 Round Bar, Stainless Steel 310S Round Bar