Stainless Steel Austenitic 1.4307 Bar
As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.
- Send E-mail: ss@gneesteel.com
Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of stainless steel austenitic 1.4307 bar in China. If you're going to wholesale high quality stainless steel austenitic 1.4307 bar made in China, welcome to get free sample from our factory. Good service and reasonable price are available.
EN 1.4307, AISI 304L stainless steel bar is a low-carbon austenitic alloy, which makes it highly weldable, formable and highly resistant to intergranular corrosion. Thestainless 304l rod is often used in the food, chemical and pharmaceutical industries. EN 1.4307 ss bar is a very common alloy and can be used in a variety of climates and environments.


Stainless steel types1.4301 and 1.4307 are also known as grades 304 and 304L respectively. Type 304 is the most versatile and widely used stainless steel. It is still sometimes referred to by its old name 18/8 which is derived from the nominal composition of type 304 being 18% chromium and 8% nickel.
1.4307 Steel Chemical Composition
| Chemical Element | % Present |
|---|---|
| Carbon (C) | 0.0 - 0.03 |
| Chromium (Cr) | 17.50 - 19.50 |
| Manganese (Mn) | 0.0 - 2.00 |
| Silicon (Si) | 0.0 - 1.00 |
| Phosphorous (P) | 0.0 - 0.05 |
| Sulphur (S) | 0.0 - 0.03 |
| Nickel (Ni) | 8.00 - 10.50 |
| Nitrogen (N) | 0.0 - 0.11 |
| Iron (Fe) | Balance |
1.4307 Stainless Steel Bar Properties
| Physical Property | Value |
|---|---|
| Density | 8.0 g/cm³ |
| Melting Point | 1450 °C |
| Thermal Expansion | 17.2 x10^-6 /K |
| Modulus of Elasticity | 193 GPa |
| Thermal Conductivity | 16.2 W/m.K |
| Electrical Resistivity | 0.72 x10^-6 Ω .m |
Spec: EN 10088-3:2005
Bar & Section - Up to 160mm Dia / thickness
| Mechanical Property | Value |
|---|---|
| Proof Stress | 175 Min MPa |
| Tensile Strength | 500 to 700 MPa |
| Elongation A50 mm | 45 Min % |
| Hardness Brinell | 215 Max HB |
Customer Visit
GNEE Steel Group is China's professional one-stop supply chain enterprise for steel products. Its stainless steel pipe production technology has reached the world's average technical level. It has been recognized by dozens of project companies and has become a star enterprise in Asia.

Over the last 30 years, we have been serving our clients, we have built a strong clientele across 32 countries and 15 industrial verticals, right from basic industries such a paper to highly demanding offshore services.
Hot Tags: stainless steel austenitic 1.4307 bar, China stainless steel austenitic 1.4307 bar suppliers, 304 304L 316 316L Stainless Round Bar, Stainless Steel 310S Round Bar, Stainless Steel 446 Round Bar, 420 Stainless H type Steel, 304 316 Steel Flat Bars With Holes
You Might Also Like
Send Inquiry