Grade 420 Stainless Steel (Cond-A, Modified)
As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.
- Send E-mail: ss@gneesteel.com
Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of grade 420 stainless steel (cond-a, modified) in China. If you're going to wholesale high quality grade 420 stainless steel (cond-a, modified) made in China, welcome to get free sample from our factory. Good service and reasonable price are available.
Grade 420 is hardenable martensitic steel. Grade 420 stainless steels have high carbon contents and are made up of at least 12 percent chromium. It is the hardest type of stainless steel with a chromium composition in this range and is available in numerous variations including condition A and modified forms. These variants have undergone additional treatments to boost or alter specific performance characteristics including strength, ductility, and machinability.




Performance Characteristics of Stainless Steel Grade 420
From a general standpoint, stainless steel grade 420 (Cond-A, Modified) is highly ductile when processed in its annealed form. It also displays outstanding oxidation resistance when it has been hardened, polished or surface-ground. Grade 430 alloys, with their higher chromium contents, are more resistant to a broader range of corrosives.
This stainless steel grade is widely used in the manufacture of shear blades, surgical instruments, and needle valves. It is also the standard alloy in stainless steel cutlery. Hardened forms of stainless steel grade 420 resist the following types of corrosive substances:
Freshwater
Alkaline materials
Mild acids
Food & organic compounds
Air
These alloys also resist wearing from heat when exposed to temperatures of up to 650° C (1200° F). They can also be machined fairly easily in their annealed state. They anneal at temperatures between 1550-1650 F (843-900 C). With that being said, they are not quite as versatile as 416-grade stainless steel alloys. When it comes to hardening, 420 grade needs to preheat, then heat to 1800-1950 F (982-1066 C), soak that temperature and air cool or quench in warm oil.
Stainless Steel Grade 420
Chemical Composition
UNS: S42000 / TYPE: 420
| Carbon (C) | Manganese (Mn) | Phosphorus (P) | Sulpher (S) | Silicon (Si) | Chrome (Cr) | |
|---|---|---|---|---|---|---|
| Min | 0.15 | 12.0 | ||||
| Max | 1.00 | 0.040 | 0.030 | 1.00 | 14.0 |
Stainless Steel Grade 420
Mechanical Composition
| Grade | UNS Number | Tensile Min (psi) | Yield Min (psi) | Elongation Min % | Reductions Min % | Hardness BHN |
|---|---|---|---|---|---|---|
| 420 | S42000 | |||||
| Cond-A | * | * | * | * | 241 Max | |
| Modified | 110,000 | 80,000 | 20 | 40 | 207-235 |
Choosing the right stainless steel alloy for a specific application can be a difficult task, given the minor variations in performance characteristics seen in both standard and variant metals. For more information about stainless steel alloy 420, or to inquire about its condition A and modified variants, please contact a knowledgeable Gnee Alloys representative today!
Message
NEED MORE INFORMATION?
FAQ
Q: What are your company's main products ?
A: Our main products are stainless steel plate/sheet, coil, round/square pipe, bar, nickel alloys, etc.
Q: How do you control quality ?
A: Mill Test Certification is supplied with shipment, Third Party Inspection is available. and we also get ISO,SGS,Alibaba Verified.
Q: What are the advantages of your company ?
A: We have many professionals, technical personnel, more competitive prices and best after-dales service than other stainless steel companies.
Q: How many coutries you already exported ?
A: Exported to more than 50 countries mainly from America, Kazakhstan, UK, Kuwait, Egypt, Turkey, Jordan,India, etc.
Q: Can you provide sample ?
A: Yes. We can provide the small samples in stock for free, as long as you contact us.Customized samples will take about 5-7 days.
Hot Tags: grade 420 stainless steel (cond-a, modified), China grade 420 stainless steel (cond-a, modified) suppliers, Stainless Steel 310S Round Bar, 420 Stainless H type Steel, 304 316 Steel Flat Bars With Holes, 304 304L 316 316L Stainless Round Bar, Stainless Steel 446 Round Bar
You Might Also Like
Send Inquiry