ASTM B408 Incoloy 800HT Round Bar Incoloy Alloy 800H Round Bar Bright Bar
video

ASTM B408 Incoloy 800HT Round Bar Incoloy Alloy 800H Round Bar Bright Bar

ASTM B408 Incoloy 800HT Round Bar Incoloy Alloy 800H Round Bar Bright Bar Incoloy 800HT Round Bars has rather equivalent chemical composition to Incoloy 800H Bars, at discrepancy just in aluminium, titanium and carbon levels in some measure. These UNS N08811 Round Bars are accessible to our valuable customers in different range of diameters, wall thicknesses and sizes in customized form and also at quite affordable rates.
Send Inquiry
Chat Now

As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.

Product Introduction

Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of astm b408 incoloy 800ht round bar incoloy alloy 800h round bar bright bar in China. If you're going to wholesale high quality astm b408 incoloy 800ht round bar incoloy alloy 800h round bar bright bar made in China, welcome to get free sample from our factory. Good service and reasonable price are available.

 

ASTM B408 Incoloy 800HT Round Bar Incoloy Alloy 800H Round Bar Bright Bar

Incoloy 800HT Round Bars has rather equivalent chemical composition to Incoloy 800H Bars, at discrepancy just in aluminium, titanium and carbon levels in some measure. These UNS N08811 Round Bars are accessible to our valuable customers in different range of diameters, wall thicknesses and sizes in customized form and also at quite affordable rates.

 

Incoloy 800H / 800HT Round Bars Specification

Specification : ASTM B 408 / ASME SB 408, AMS 5766

Dimensions : ASTM, ASME and API

Size : 5 mm To 500 mm Dia in 100 mm TO 6000 mm Length available with NACE MR 01-75.

Length : 100 mm To 3000 mm Long & Above

Finish : Bright, Polish & Black

Grade : Incoloy 800H – UNS N08810, Incoloy 800HT / HT – UNS N08811

Form : Round, Square, Hex (A/F), Rectangle, Wire (Coil Form), Wire-mesh, Billet, Ingot, Forging Etc.

Our Incoloy 800H / 800HT Round Bars conforms to NACE MR0175/ISO 15156

 

ASTM B408 Incoloy 800H / 800HT Bars Equivalent Grades

 

STANDARD WERKSTOFF NR. UNS GOST AFNOR JIS BS EN OR
Incoloy 800H 1.4958 / 1.4876 N08810 ЭИ670 Z8NC33-21 NCF 800H NA 15(H) X5NiCrAlTi31-20 XH32T
Incoloy 800HT 1.4859 / 1.4876 N08811 ЭИ670 - NCF 800HT NA 15(HT) X8NiCrAlTi32-21 XH32T

 

Incoloy 800H / 800HT Round, Bright, Hex, Threaded Bar Chemical Composition

 

Grade Ni Cr Fe Si Ti Cu Mn C S Al
Incoloy 800H 30.0 - 35.0 19.0 - 23.0 39.5 min 1.0 max 0.15 - 0.60 0.75 max 1.5 max 0.05-0.1 0.015 max 0.15 -0.60
Incoloy 800HT 30.0 - 35.0 19.0 - 23.0 39.5 min 1.0 max 0.25-0.60 0.75 max 1.5 max 0.06-0.1 0.015 max 0.85-1.20

 

Incoloy 800H / 800HT Round Bars Mechanical Properties

 

Density Melting Point Tensile Strength Yield Strength (0.2%Offset) Elongation
7.94 g/cm3 1350-1400℃ Psi – 75,000 , MPa – 500 Psi – 30,000 , MPa – 200 30 - 35 %

 

Types Of Available Products AISI, ASTM, DIN, ASME Incoloy 800H / 800HT Round Bars
ASTM B408 Incoloy 800HT Round Bar Incoloy Alloy 800H  Round Bar Bright Bar 0ASTM B408 Incoloy 800HT Round Bar Incoloy Alloy 800H  Round Bar Bright Bar 1ASTM B408 Incoloy 800HT Round Bar Incoloy Alloy 800H  Round Bar Bright Bar 2ASTM B408 Incoloy 800HT Round Bar Incoloy Alloy 800H  Round Bar Bright Bar 3

Hot Tags: astm b408 incoloy 800ht round bar incoloy alloy 800h round bar bright bar, China astm b408 incoloy 800ht round bar incoloy alloy 800h round bar bright bar suppliers, 304 316 Steel Flat Bars With Holes, 420 Stainless H type Steel, Stainless Steel 446 Round Bar, Stainless Steel 310S Round Bar, 304 304L 316 316L Stainless Round Bar