310MoLN 725LN Urea Grade S31050 Ss Round Bars Ultra 725LN EN 1.4466 ASTM UNS S31050
video

310MoLN 725LN Urea Grade S31050 Ss Round Bars Ultra 725LN EN 1.4466 ASTM UNS S31050

Stainless steel grade 310MoLN is a fully austenitic stainless steel that does not have intermetallic phases such as intergranular carbide precipitations. The 310MoLN steel grade has an optimized chemical composition designed specifically for applications in urea plants. The nitrogen in the chemical composition helps to stabilize and strengthen the austenitic phase. This material provides improved corrosion-resistance in urea carbamate environments such as high-pressure strippers.
Send Inquiry
Chat Now

As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.

Product Introduction

Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of 310moln 725ln urea grade s31050 ss round bars ultra 725ln en 1.4466 astm uns s31050 in China. If you're going to wholesale high quality 310moln 725ln urea grade s31050 ss round bars ultra 725ln en 1.4466 astm uns s31050 made in China, welcome to get free sample from our factory. Good service and reasonable price are available.

 

310MoLN (725LN) Stainless Steel Bar Urea Grade S31050 Round Bar Ultra 725LN EN 1.4466, ASTM UNS S31050

 

310MoLN (725LN)

Introduction

A-one Alloy supplies high quality 310MoLN bars and pipes.

Stainless steel grade 310MoLN is a fully austenitic stainless steel that does not have intermetallic phases such as intergranular carbide precipitations. The 310MoLN steel grade has an optimized chemical composition designed specifically for applications in urea plants. The nitrogen in the chemical composition helps to stabilize and strengthen the austenitic phase. This material provides improved corrosion-resistance in urea carbamate environments such as high-pressure strippers.

Density: 7.9g/cm3

Character

Very good corrosion resistance to carbamide synthesis.

Good corrosion resistance to intergranular corrosion.

Application

Production of carbamide.

Equal grades

UNS S31050, EN 1.4466, 00Cr25Ni20Mo2N, 25-22-2, X1CrNiMoN25-22-2

Chemical composition

C≤0.030, Mn≤2.00, P≤0.030, S≤0.015, Si≤0.50, Ni=20.5~23.5, Cr=24.0~26.0, Mo=1.6~2.6, N=0.09~0.15, Fe=reminder

Standards

ASTM A240 Standard Specification for Chromium and Chromium-Nickel Stainless Steel Plate, Sheet, and Strip for Pressure Vessels and for General Applications

ASTM A182-A182M-13 Standard Speci?cation for Forged or Rolled Alloy and Stainless Steel Pipe Flanges, Forged Fittings, and Valves and Parts for High-Temperature Service

Product forms available at A-one Alloy

Bar, plate, sheet, tube, forging

Delivery

as PO

 

310MoLN 725LN Urea Grade S31050 Ss Round Bars Ultra 725LN EN 1.4466 ASTM UNS S31050 0310MoLN 725LN Urea Grade S31050 Ss Round Bars Ultra 725LN EN 1.4466 ASTM UNS S31050 1310MoLN 725LN Urea Grade S31050 Ss Round Bars Ultra 725LN EN 1.4466 ASTM UNS S31050 2310MoLN 725LN Urea Grade S31050 Ss Round Bars Ultra 725LN EN 1.4466 ASTM UNS S31050 3310MoLN 725LN Urea Grade S31050 Ss Round Bars Ultra 725LN EN 1.4466 ASTM UNS S31050 4

Hot Tags: 310moln 725ln urea grade s31050 ss round bars ultra 725ln en 1.4466 astm uns s31050, China 310moln 725ln urea grade s31050 ss round bars ultra 725ln en 1.4466 astm uns s31050 suppliers, 420 Stainless H type Steel, Stainless Steel 310S Round Bar, 304 304L 316 316L Stainless Round Bar, 304 316 Steel Flat Bars With Holes, Stainless Steel 446 Round Bar

Send Inquiry

whatsapp

Phone

E-mail

Inquiry