Jan 29, 2024 Leave a message

What Material Is Monel400 Made Of?

What material is Monel400 made of?

 

Monel400 copper-nickel alloy-corrosion-resistant nickel alloy

Monel400 copper-nickel alloy has low strength in the annealed state, therefore, in the rolled state, it exhibits a higher degree of strength. Alloy 400 is a ductile, corrosion-resistant copper-nickel alloy. Alloy 400 is widely used in oxidizing, neutral and reducing environments. It is also used in underwater environments and chloride solutions that cannot be oxidized.

Monel400 copper-nickel alloy (UNSN004400) specifications

Monel400 copper-nickel alloy is a nickel-based alloy that can withstand various corrosive environments.

General Properties Monel Alloy, Monel 400 (UNSN04400) is a soft copper-nickel alloy that is resistant to various corrosive environments. This alloy is often named for use in mild oxidizing environments, neutral environments, and waning environments. Another area of application is in marine environments and other non-oxidizing chloride solutions.

What material is Monel400 made of?

What material is Monel400 made of?

The alloy has a long history as a corrosion-resistant material, dating back to the 20th century. At the time, it was intended to be used as a nickel metal with a high copper content. Roughly equal amounts of nickel and copper in the metal are now officially specified as a requirement for production of the alloy.

As a commercially available pure nickel, Monel400 copper-nickel alloy has low strength under annealed conditions. For this reason, various tempering methods must be used to increase the strength of the material.

Application areas

Marine and Chemical Processing Equipment

Valves, water pumps, propeller shafts

Fasteners for marine fixtures

Gasoline and clean water tanks

Processing vessels and pipes

heat exchanger

Standards American Society for Testing and Materials.........B127 American Society of Mechanical Engineers.........SB127 US Army Standards...................... ....4544 Federal or Military Standard....QQ-N-281

Corrosion-resistant Monel 400 copper-nickel alloy is more corrosion-resistant than commercially available pure nickel (UNSN02200) in weakened environments and more corrosion-resistant than refined copper alloys in oxidizing conditions. In suitably weakened acid, neutral or alkaline solutions, Monel 400 copper-nickel alloy may be considered for use. The alloy is corrosion resistant to most alkalis, salts, organic compounds, and atmospheric conditions. Although the material has experienced corrosion stress cracking under high temperatures, high stress, and high corrosion concentrations, Monel400 copper-nickel alloy can be considered for use under cooler alkali corrosion conditions. The alloy is used in weak acids such as sulfur and hydrogen chloride, especially when there is no ventilation and no oxides.

Monel400 copper-nickel alloy is particularly resistant to chloride stress cracking corrosion. Its main application environment is various types of water including seawater and salt water.

Monel400 copper-nickel alloy is corroded when sulfur-containing gas exceeds 700 degrees Fahrenheit (371 degrees Celsius); when molten sulfuric acid exceeds approximately 500 degrees Fahrenheit (260 degrees Celsius), it can corrode Monel400 copper-nickel alloy.

 

Send Inquiry