Inconel 718 forged round bar, Φ160 mm, end face marked with grade and UNS number.
Inconel 718 AMS 5662 vs AMS 5663 is a comparison between two procurement specifications that describe one alloy, UNS N07718, in three product forms: bar, forgings and rings. Both documents share a single chemistry and a single strengthening mechanism.
The contrast lies in the condition the mill ships. AMS 5662 material leaves the works solution treated and is aged later; AMS 5663 material leaves the works already aged. Buyers sometimes treat the two as interchangeable grades, and they are not interchangeable without a check of the delivery condition. The specification choice fixes who runs the precipitation hardening cycle and in which condition strength is demonstrated.
Both documents are read alongside ASTM B637, which covers the same alloy and the same product forms in either condition. Procurement therefore comes down to three questions: which condition ships, who performs the aging, and whether the part is machined before or after hardening.

What Is AMS 5662?
AMS 5662 is the specification for Inconel 718 bar, forgings and rings supplied in the solution treated, precipitation hardenable condition. The mill performs the solution treatment at 1775°F (968°C) and ships the material without aging, so precipitation hardening is left to the purchaser after machining or forming. Because the alloy is still workable at delivery, this stock suits parts that need substantial cutting, forming or welding before they reach final strength.
What Is AMS 5663?
AMS 5663 covers the same Inconel 718 bar, forgings and rings in the solution treated and precipitation heat treated condition. The mill completes the double aging cycle before shipment: 1325°F ± 25 (717°C) for 8 hours, furnace cooling to 1150°F ± 25 (621°C) to a cumulative 18 hours, then air cooling. Parts cut from this stock arrive at final strength, so machining allowances and tool paths must suit the hardened condition.

AMS 5662 VS 5663 Inconel 718:Comparison of Chemical Composition
| Item | AMS 5662 | AMS 5663 |
|---|---|---|
| Alloy | Inconel 718 / UNS N07718 | Inconel 718 / UNS N07718 |
| Scope | Bars, forgings, rings | Bars, forgings, rings |
| Chemistry | Identical (Ni 50–55, Cr 17–21, Nb 4.75–5.5, Mo 2.8–3.3, Ti 0.65–1.15, Al 0.2–0.8) | Identical |
| Melt practice | Consumable electrode VIM/VAR, premium quality | Same |
| Heat treatment delivered | 968 °C (1775 °F) solution treat + rapid cool | Solution treat + double age (718 °C/8 h, furnace cool, 621 °C/8 h) |
| Delivery hardness | Soft, typically ≤ 250 HB | Aged, typically 36–40 HRC |
| Room-temp tensile (min) | No aged-strength requirement | 1240 MPa (180 ksi) |
| Yield (0.2%, min) | Not specified in aged state | 1034 MPa (150 ksi) |
| Elongation (min) | Not specified in aged state | 12% |
| Typical use state | Part still needs aging | Part used as delivered |
Key point: the physical difference is one heat-treatment step. Everything else - composition, cleanliness, grain control, testing method - is effectively the same.

PMI spectrometer verification of Alloy 718 chemistry before dispatch.
AMS 5662 vs AMS 5663: Key Differences in Mechanical Properties
The measurable gap between the two specifications follows from one point: AMS 5663 properties are accepted in the aged condition as shipped, while AMS 5662 properties are demonstrated on specimens aged after solution treatment, not on the as-shipped condition.
| Comparison point | AMS 5662 | AMS 5663 |
|---|---|---|
| Delivery condition | Solution treated, precipitation hardenable; shipped unaged | Solution treated and precipitation heat treated; shipped aged |
| Heat treatment | 1775°F (968°C) solution treatment at the mill; aging performed after delivery | 1775°F (968°C) solution treatment, then 1325°F (717°C) for 8 hours, furnace cool to 1150°F (621°C), 18 hours cumulative, air cool |
| Typical use | Parts machined, formed or welded before aging | Fasteners and components installed without further heat treatment |
Standards and Equivalents: AMS 5662, AMS 5663 and ASTM B637
Four standards govern this alloy in bar, forgings and rings. The list below adds the UNS designation and one cross-reference designation, then states what each entry covers and where it diverges.
- UNS N07718 - the unified numbering system designation shared by every document on this page.
- AMS 5662 - bar, forgings and rings; solution treated at 1775°F (968°C); precipitation hardenable, aged after delivery.
- AMS 5663 - bar, forgings and rings; solution treated at 1775°F (968°C) and double aged before shipment.
- AMS 5664 - bar, forgings and rings; 1950°F (1066°C) high temperature solution treatment, then 1400°F (760°C) for 10 hours, furnace cool to 1200°F (649°C) to a cumulative 20 hours, air cool; written for heavy sections where creep rupture ductility and notch toughness govern.
- ASTM B637 - bar, forgings and forging stock for UNS N07718, issued with a solution treated and precipitation hardenable condition and with a solution plus precipitation heat treated condition.
- GH4169 - Chinese designation for the same alloy, recorded for cross-reference only and not a substitute document.
AMS 5662 Equivalent Specifications
An AMS 5662 equivalent is the same UNS N07718 material certified to another document in a comparable condition, not a different grade. When a drawing cites an equivalent standard, confirm the delivery condition on the purchase order before releasing the heat, because one alloy name can be supplied aged or unaged.
AMS 5663 Equivalent ASTM
ASTM B637 covers the same product forms in both delivery conditions, so the correspondence runs in pairs. AMS 5662 matches the ASTM B637 solution treated, precipitation hardenable state; AMS 5663 matches the ASTM B637 solution and precipitation heat treated state. Cross-check each purchase order against the condition actually required.
GNEE STEEL Inconel 718 Manufacturing and Heat Treatment
Heat treatment is where the two specifications separate on the shop floor. Forging practice and ring rolling set the prior structure, the final solution treatment restores it, and aging develops strength. The three stages below apply to all three product forms.
Solution Treated Condition (AMS 5662)
Solution treatment holds the material at 1775°F (968°C) to dissolve the strengthening phases and any delta phase present, then cools it fast enough to retain a supersaturated matrix. The mill certifies that condition and ships without further thermal work. Hardness in this state is comparatively low, which keeps machining, forming and welding practical. Precipitation hardening stays open so it can follow the purchaser's process route.
Double Aging Cycle (AMS 5663)
AMS 5663 adds the full precipitation hardening cycle at the mill. The load is held at 1325°F ± 25 (717°C) for 8 hours, furnace cooled to 1150°F ± 25 (621°C) at a controlled rate of about 100°F (56°C) per hour, held to a cumulative aging time of 18 hours, then air cooled. The two step hold grows gamma double prime and gamma prime precipitates to a controlled size, which raises proof strength while keeping ductility and notch toughness.
Precipitation Hardening After Delivery
AMS 5662 stock can be age hardened by the purchaser. Machining, forming or welding is completed first and the aging cycle is applied afterwards, most often the same double aging sequence used for AMS 5663. Two conditions apply: the part must be brought to temperature with uniform section control, and acceptance testing must be planned after aging, because as-delivered properties do not represent service strength.
Alloy 718 Applications
Alloy 718 combines elevated temperature strength with corrosion resistance and low temperature toughness, which is why one specification family serves gas turbine, aerospace and oilfield duty.
Gas Turbine and Aeroengine Components

Gas turbine applications of Alloy 718. Illustration; actual part geometry per drawing.
Gas turbine disc material and aeroengine turbine shaft alloy draw on Alloy 718 for the same reason: high proof strength at temperature with workable ductility and fatigue resistance. Compressor discs, spacers, shafts and forged rings are ordered to AMS 5663 where finish machining is light, or to AMS 5662 where heavy machining comes before aging.
High Temperature Fasteners
High temperature fasteners in Inconel 718 depend on the aged condition. Fastener stock is usually ordered in the aged condition so that strength and hardness acceptance are settled before blanks are cut and threaded. The mapping for fastener drawings and for other part families is set out in the next section.
Downhole Tools and Wellhead Components
Downhole tools and wellhead components use the alloy for sour service resistance and for the mechanical loads of completion hardware. NACE MR0175 / ISO 15156-3 covers the alloy for sour oil and gas service, subject to hardness control and to the temperature and environmental limits written into that standard. Aged stock shortens the heat treatment route for these parts.
GNEE STELL Inconel 718 suppliers
At GNEE, Inconel 718 is available in various forms to meet diverse industrial needs:
Plates and Sheets (cold rolled and hot rolled)
Bars and Rods (round, square, hexagonal)
Tubes (seamless and welded)
Wires and Strips (for springs, fasteners, electrical applications)
Forgings and Custom Parts (according to drawings or specifications)
Specifications: UNS NO7718, WNR 2.4668, AFNOR NC19FeNb, JIS NCF 718, GOST ХН75МБТЮ, EURONORM NiCr22Mo9Nb, OR ЭИ602, BS NA 21.
Temperature Range: -423°F to 1300°F.
Testing and Documentation: Mill Test Certificates, EN 10204 3.1, Chemical Reports, Mechanical Reports, Destructive Testing Reports, Non-Destructive Testing Reports, PMI Test Reports, Visual Inspection Reports, Third-Party Inspection Reports, NABL Certified Laboratory Reports.
Packaging: Wooden crates, bubble wrap, steel strapping, or packaged according to customer requirements.




FAQ:
What is the difference between AMS 5662 and AMS 5663?
AMS 5662 covers Inconel 718 bar, forgings and rings in the solution treated condition, while AMS 5663 covers the same product forms in the fully precipitation heat treated, or aged, condition. AMS 5662 also allows the purchaser to perform the final aging, so the two specifications accept mechanical properties in different conditions.
What condition is Inconel 718 delivered in under AMS 5662?
Under AMS 5662, Inconel 718 bar, forgings and rings are delivered solution treated at 1775°F (968°C) and are precipitation hardenable, so final aging happens after delivery. Chemistry is identical to AMS 5663; only the heat treatment condition differs.
Does AMS 5663 include precipitation aging?
Yes. AMS 5663 material is solution treated and then precipitation heat treated by double aging, at 1325°F (717°C) for 8 hours and then 1150°F (621°C), for 18 hours total, before air cooling. This is the standard double aging cycle referenced in the specification.
Which AMS spec should I order for Inconel 718 fasteners?
Order Inconel 718 fasteners to AMS 5663, because the age hardened delivery condition already provides the high strength fasteners need, while AMS 5662 suits parts machined or formed before aging. Confirm final hardness and strength acceptance with your fastener drawing.
What is UNS N07718?
UNS N07718 is the unified numbering system designation for Inconel 718, a nickel chromium iron alloy strengthened by precipitation hardening for gas turbine, aerospace and oilfield components. Both AMS 5662 and AMS 5663 designate this same UNS number.