Detailed explanation of Monel 400 (Monel400, N04400) alloy material knowledge
Monel 400 (N04400) nickel-copper alloy material properties:
Monel 400 (Monel 400, N04400) is a nickel-copper alloy with first-class corrosion resistance to a variety of reducing media, and also has certain mechanical properties. Monel400 has particularly excellent corrosion resistance against air-free hydrofluoric acid, neutral and alkaline salt solutions.
Monel 400 is used for uranium refining and isotope separation in nuclear fuel production. It is a standard material for the concentration and crystallization of salt solutions, vinyl chloride monomer (VCM) production, MDI and TDI production, and petroleum refining. Monel 400 is also used to manufacture feedwater heaters and steam generator heat transfer tubes, sheathed pipes and platform steel columns used in offshore oil and gas production. Monel 400 alloy is certified for use in pressure vessels with operating temperatures between -10 and 425°C (18 and 797°F).
1. Monel400 alloy has good corrosion resistance against stress corrosion caused by aluminum elements
2.Monel400 still maintains excellent strength at low temperatures
3.Monel400 (N04400) is easier to process than other high alloy materials


Certified for use in pressure vessels from -10 to 425°C (14 to 797°F) according to VdTÜV Material Sheet No. 263, with maximum service temperatures up to 480°C (896°F) according to the ASME Boiler and Pressure Vessel Code ).
Corrosion resistance of Monel 400 (N04400) material:
Monel 400 (Monel 400, N04400) has excellent corrosion resistance to neutral salts and alkaline salts, so it has long been a standard material in the field of salt production. N04400 is one of the few materials that can come into contact with fluorine, hydrofluoric acid, hydrogen fluoride and their compounds. The material has excellent resistance to corrosion by alkaline media. It also performs very well in seawater and has better cavitation resistance than copper-based alloys. Monel400 Monel alloy has good corrosion resistance to dilute mineral acids (such as sulfuric acid and hydrochloric acid) under non-ventilated conditions.
Since Monel 400 (Monel 400, N04400) does not contain chromium, the corrosion rate will increase significantly under oxidizing conditions. Although Monel 400 is resistant to stress corrosion cracking, stress cracking can occur when exposed to mercury-containing or moist hydrofluoric acid vapors. If used under the above conditions, stress relief annealing must be performed.
Common application areas of Monel 400, Monel 400, and N04400 include:
1. Feed water and steam generator heat transfer tubes in power plants
2. Brine heaters and recompression evaporators in salt plants
3. Sulfuric acid and hydrofluoric acid alkylation
4. Heat exchangers in the chemical industry
5. Electroplating equipment for mineral oil distillation plants
6. Splash zone lining of offshore platform
7. Ship impellers and pump shafts
8. Refineries that produce nuclear fuel
9. Pumps and valves on production lines for tetrachlorethylene (perchlorethylene) and chlorinated plastics
10. Heating tube for monoethanolamine (MEA)
In addition, Monel 400, Monel 400, and N04400 are also used in sour gas-resistant components for oil and natural gas production.