Monel 400 alloy implementation standards, mechanical properties and chemical composition
Monel 400 alloy introduction:
NCu30 (N04400), NCu30Fe, is a kind of chemical solvent that can be used in seawater, chemical solvents, ammonia sulfur chloride, hydrogen chloride, various acidic media such as sulfuric acid, hydrofluoric acid, hydrochloric acid, phosphoric acid, organic acids, alkaline media, salts and molten salts. A nickel-based alloy material with good corrosion resistance, Monel 400 alloy also has good mechanical properties, a wide range of use temperatures from low to high temperatures, good welding performance and medium and high strength.


Usage: Used in chemical and petrochemical industries, as well as marine development and other fields
Implementation standards: GB/T5235-2007
GB/T21653-2008
GB4435-84
GB/T2072-2007
Q/SH25-2010
Q/SH70-2010
Monel 400 (Ni68Cu28Fe)
Monel 400 is a nickel-copper alloy with large usage, wide range of uses, good performance and high corrosion resistance. The chemical composition is mainly composed of Cu30% and Ni65%, plus a small amount of Fe (1-2%). The organizational structure is single-phase austenite.
Monel 400 has good welding performance. TIG and MIG methods can be used. Monel 60 welding wire can be used: or manual arc welding and submerged arc welding: when welding with carbon steel and low alloy steel, Monel 190 welding rod can be used.
Monel 400 is mainly used in chemical and petrochemical industries as well as marine development. Manufactures various heat exchange equipment, boiler feed water heaters, petroleum and chemical pipelines, containers, towers, tanks, valves, pumps, reactors, shafts, etc.