Sep 05, 2025 Leave a message

Detailed Introduction Of Inconel 718 Alloy Fasteners

 
 
 
Detailed introduction of Inconel 718 alloy fasteners
Detailed introduction of Inconel 718 alloy fasteners
01.

Detailed introduction of Inconel 718 alloy fasteners

Inconel 718 Fasteners are high-strength, nickel-based, superalloy fasteners commonly used in demanding applications due to their excellent mechanical properties and corrosion resistance at high temperatures (up to 1300°F). These fasteners exhibit precipitation hardening properties, achieving high yield, tensile, and creep-rupture strengths through specific heat treatments. Key applications include the aerospace, oil and gas, and power generation industries, where their ability to maintain strength under pressure and extreme temperatures is crucial for safety and performance.

02.

What is the strength of Inconel 718 bolts?

185-220 ksi
Twice as strong as its sister alloy, Inconel 625, Inconel 718 is known for its exceptionally high strength after age hardening (185-220 ksi tensile strength). Inconel 718 bolts maintain their strength even when subjected to pressure and temperatures up to 1300°F (700°C).

Inconel 718 Bolts

Specifications of Inconel 718 Fasteners

Standard UNS Werkstoff Nr.
Inconel 718 N07718 2.4668

 

Mechanical & Physical Properties Of Inconel 718 Fasteners

Density Melting Point Tensile Strength Yield Strength (0.2%Offset) Elongation
8.2 g/cm3 1350 °C (2460 °F) Psi – 135,000 , MPa –930 Psi – 70,000 , MPa – 482 45 %


INCONEL 718 FASTENERS CHEMICAL COMPOSITION

Grade Cr Fe Ni C Mn Cu Si S
Inconel 718 17-21 Bal 50-55 0.08 max 0.35 max 0.3 max 0.35 max 0.015 max

 

Inconel 718 Fastener Applications
Aerospace: Used in the manufacture of critical components for aircraft and space exploration, where high strength and reliability are essential under extreme conditions.
Oil and Gas: Used in downhole tools and pipelines, which often require high pressure and corrosive environments.
Power Generation: Used in turbines and other power generation equipment operating at high temperatures.
Automotive: Used in the manufacture of high-performance automotive components.

 

Benefits of Inconel 718 Fasteners
Enhanced Safety: Its ability to withstand extreme conditions reduces the risk of failure in critical systems.
Extended Service Life: The alloy's corrosion and high-temperature resistance extend component life.
Versatility: Suitable for a variety of demanding applications across multiple industries.

Gnee Steel

 

About Gnee Steel

Gnee Steel specializes in the production and sale of various nickel-based alloys, including Nickel 201, Nickel 202, Hastelloy C-276, Hastelloy C-22, Hastelloy B, Hastelloy C-4, Inconel Alloy 600, Inconel 625, Inconel 718, Inconel X-750, Incoloy Alloy 800, Incoloy 800H/HT, Incoloy 825, Monel Alloy 400, Monel K500, and high-temperature alloys. Gnee Steel's products are widely used in aerospace, chemical, electric power, automotive, and nuclear energy applications, and we can provide customized alloy solutions tailored to customer needs. For alloy pricing inquiries or customized alloy solutions, please contact us for a quote at ss@gneemetal.com.

Send Inquiry

whatsapp

Phone

E-mail

Inquiry