Can duplex stainless steels be stress relieved?
Possibility of stress relieving
Duplex stainless steels may have residual stresses in cold forming, machining or assembly after welding. Typically, these stresses are reduced by:
Heating: heating the metal to an appropriate temperature.
Holding: holding at this temperature for a period of time to reduce residual stresses.
Slow cooling: to minimize the development of further residual stresses.


Specialities of duplex stainless steels
For duplex stainless steels, due to their metallurgical properties, they are prone to the formation of deleterious and unwanted phases at temperatures usually considered for stress relieving. As one handbook states: "No satisfactory temperature below the solution annealing temperature can be used for stress relieving without the danger of forming intermetallic phases that reduce corrosion resistance and reduce toughness."
Stress Relief of Alloy 2205
For Alloy 2205, the lowest solution temperature mentioned is 1040°C. More critically, however, cooling from this temperature requires rapid quenching, which introduces new considerations such as deformation and further residual stresses. Similar situations exist for other duplex stainless steels.
Practical considerations
In practice, it may not be possible to stress relieve duplex stainless steel products and equipment, but solutions can be found on a case-by-case basis, such as considering the motivation for such a heat treatment operation in the first place.