Jun 05, 2025 Leave a message

Problems With Machining Nickel Alloys

Problems with machining nickel alloys

 

 

Nickel-based high-temperature and corrosion-resistant alloys can be difficult to machine because they harden quickly, may weld to the cutting tool surface, generate high heat during cutting, and offer higher resistance to metal removal due to their high shear strength.

Here are some tips and suggestions for machining nickel alloys mentioned in the article:

Why is nickel difficult to machine?
Nickel can be difficult to machine because the correct approach or tooling is not taken. Some people mistakenly treat nickel as a high-strength, high-resistance metal.

Problems with machining nickel alloysProblems with machining nickel alloys

Tips for machining nickel alloys
Tool selection: Due to the unique properties of nickel alloys, you may find that tools become dull quickly. Therefore, tools need to be resharpened or replaced regularly. If possible, it is recommended to use more expensive C-grade inserts.

Drilling factors: When using CNC machines and plunge drills, it is best to select the same speed (SFM) when facing, boring, or turning any particular alloy. The recommended feed rate is 0.002 inches per revolution.

Turning Tips: If using steel cutting tools, speeds of up to 35 ft/min may be achieved, with feeds of about 0.010 to 0.12 in. per revolution. High-speed tools may be more effective than carbide tools when cutting off.

Reaming Operations: Speeds here should be half of drilling speeds, with feeds about three times as fast. Short tools with edge relief angles between 5 and 8 degrees are recommended.

Tapping Situations: It is recommended to select a tapping drill that is slightly larger than a standard drill, as metal may flow into the cut.

Use of Coolants and Lubricants: Heat buildup is the primary cause of distortion. A careful trial process is often required to find the best solution for your specific situation. In tapping and heavy-duty drilling situations (involving large diameters or deep holes), a light-viscosity but heavy-duty petroleum-based cutting oil is usually a good choice. For CNC equipment and engine lathes, water-soluble vegetable oil-based fluids may be found to work well.

Consider Capacity: Boring and facing of nickel alloys can be performed on nearly any appropriate machine. You will make individual choices based on specific factors such as depth of cut, speed, tooling and feeds. Larger holes and tapping will require a higher degree of machine power and strength.

Send Inquiry