Jun 05, 2025 Leave a message

Alloy 904L Alloy Pipe

Alloy 904L Alloy Pipe

 

 

Product Specifications
Material: 904L Alloy Pipe
Standards: ASTM A213, A269 / ASME SA213 AVG WALL / NACE MR0175, MR0103

Size Range:
Outside Diameter (OD): 0.250"–1.000"
Wall Thickness: .035"–.065"

Chemical Requirements
Alloy 904L (UNS N08904):
Carbon (C): 0.020% max
Manganese (Mn): 2.00% max
Phosphorus (P): 0.040% max
Sulfur (S): 0.030% max
Silicon (Si): 1.00% max
Chromium (Cr): 19.0–23.0%
Nickel (Ni): 23.0–28.0%
Molybdenum (Mo): 4.0–5.0%
Nitrogen (N): 0.10% maximum
Copper (Cu): 1.00–2.00%

Alloy 904L Alloy PipeAlloy 904L Alloy Pipe

Mechanical Properties
Yield Strength: 31 ksi minimum
Tensile Strength: 71 ksi minimum
Elongation: 35% minimum
Hardness: 90 HRB maximum (Rockwell B scale)

Typical Applications
Acid Production
Fertilizer Processing
Oil Refining
Gas Scrubbers
Pulp and Paper Processing
Seawater Cooling Equipment
Controls and Instrumentation

Physical Properties
904L Alloy: is a low carbon, high alloy austenitic stainless steel with copper added to give it superior corrosion resistance to conventional chromium-nickel stainless steels, especially in sulfuric, phosphoric, and acetic acid environments.

Fabrication Properties
904L Alloy is nonmagnetic in all conditions and has excellent formability and weldability. The austenitic structure also gives this alloy excellent toughness at low temperatures.