ASTM B514 Incoloy 800H welded boiler tubes are made from a high-performance nickel-iron-chromium alloy. They offer excellent high-temperature strength, corrosion resistance, and creep resistance, making them ideal for use in extreme environments such as power generation and petrochemical processing. Key properties include high-temperature strength up to 982°C (1800°F), resistance to oxidation and carburization, and good weldability. The "H" designation indicates a higher carbon content, resulting in improved high-temperature mechanical properties and creep resistance compared to standard Incoloy 800.

What are the ASTM specifications for Incoloy 800?

The chemical composition of INCOLOY 800HT alloy falls within the range of 800H alloy and requires a heat treatment temperature of at least 2100°F (1149°C). The carbon content is 0.06% to 0.10% (compared to 0.05% to 0.10% for 800H alloy), and the aluminum and titanium content is 0.85% to 1.20% (compared to 0.30% to 1.20% for 800H alloy).
Chemical Composition %
| B514 | Ni | Cr | FeA | Mn | C | Cu | Si | S | Al | Ti |
| NO8810 | 30.0-35.0 | 19.0-23.0 | 39.5min | 1.5max | 0.05-0.10 | 0.75max | 1.0 | 0.015 | 0.15-0.60 | 0.15-0.60 |
Mechanical Property NO8810
| Condition (Temper) | Tensile Strength min | Yield Strength, 0.2% offset min | Elongation |
| annealed | 65000 psi,450 MPa | 25000 psi,170 MPa | 30% |
Materials and Properties
Alloy: Incoloy 800H, a nickel-iron-chromium alloy designed for demanding applications.
Composition: A higher carbon content than the base Incoloy 800 alloy improves creep and rupture strength at elevated temperatures.
High-Temperature Performance: Demonstrates excellent strength and resistance to deformation and fracture at temperatures up to 982°C (1800°F).
Corrosion Resistance: Provides excellent resistance to oxidation, carburization, and general corrosion in aggressive chemical and high-temperature environments.
Weldability: Excellent weldability makes it a top choice for complex piping systems.
Applications
Chemical Processing: Used in reactors, heat exchangers, and piping systems where high-temperature strength and corrosion resistance are critical.
Power Generation: Used in various components within power plants.
Petrochemical Refining: Widely used in furnace components, heat exchangers, and other critical systems.
Industrial Furnaces: Suitable for heat-treating equipment such as baskets, trays, and fixtures.
Key Benefits of Incoloy 800H
Increased Creep Strength: The higher carbon content in 800H alloy provides superior creep-rupture performance compared to standard 800 alloy.
Thermal Stability: Maintains its strength and ductility for extended periods at elevated temperatures.
Versatility: Withstands thermal cycling without significant performance degradation.
High Performance: It is the preferred choice for critical piping systems where reliability under extreme conditions is paramount.

Gnee Steel specializes in the production and sale of various nickel-based alloys, including Nickel 201, Nickel 202, Hastelloy C-276, Hastelloy C-22, Hastelloy B, Hastelloy C-4, Inconel Alloy 600, Inconel 625, Inconel 718, Inconel X-750, Incoloy Alloy 800, Incoloy 800H/HT, Incoloy 825, Monel Alloy 400, Monel K500, and high-temperature alloys. Gnee Steel's products are widely used in aerospace, chemical, electric power, automotive, and nuclear energy applications. We also offer customized alloy solutions tailored to customer needs. For alloy pricing inquiries or customized alloy solutions, please contact us for a quote at ss@gneesteel.com.