ASTM B407 UNS N08800 Nickel alloy pipes for seawater desalination
ASTM B407 UNS N08800 nickel alloy tubing is suitable for seawater desalination due to its excellent resistance to high-temperature corrosion, oxidation, and carburization, as well as good resistance to corrosion in aqueous media. They are stable at high temperatures, making them ideal for applications such as heat exchangers and process piping, especially in harsh environments where standard steel cannot withstand them. While not recommended for applications subjected to extreme stresses, their ease of welding and forming makes them a widely used material in this field.
What are the specific specifications of Incoloy 800?
The chemical composition of Incoloy 800HT alloy is limited to the range of 800H alloy and requires heat treatment at at least 2100°F (1149°C). Its carbon content is 0.06% to 0.10% (0.05% to 0.10% for 800H alloy), and its Al + Ti content is 0.85% to 1.20% (0.30% to 1.20% for 800H alloy).

ASTM B407 UNS N08800 Alloy 800 Type 1.4876 Nickel Alloy Seamless Tube for Seawater Desalination
The primary chemical composition of ASTM B407 UNS N08800 steel alloy is nickel, comprising 52%. It also contains 19% chromium and 18% iron. Incoloy 800 nickel alloy tubes exhibit excellent corrosion resistance, showing strong resistance to corrosion in acidic environments. ASTM B407 UNS N08800 (Alloy 800) nickel alloy seamless tubes are designed to resist oxidation and carburization, exhibiting excellent overall corrosion resistance. Incoloy 800 nickel alloy is a widely used material for manufacturing high-strength, oxidation-resistant, carburization-resistant, and other equipment susceptible to the harmful effects of high temperatures. ASTM B407 Incoloy 800 seamless steel tubes are a high-strength steel designed for excellent strength and load-bearing capacity.
Specification:
| Secification | ASTM B407, ASME SB407 |
| Material Grades | Incoloy 800 / Incoloy 800H / Incoloy 800HT / Incoloy 825 / UNS NO8800 / UNS NO8810 / UNS NO8811 / UNS NO8825 |
| Type | Cold Drawn Seamless |
| Outer Diameter Size | 1/2" to 24" |
| Wall Thickness | SCH10 to SCH160 |
| Length | 6 Meters, Or Customized Size |
| Pipes Ends | Plain Ends, Beveled Ends |
| Delivery Conditions | As Rolled, Cold Drawn, Hot Finish, Stress Relieved, Annealed, Hardened, Tempered |
| Coating | Electropolish, Mechanical Polish, Satin Finish, Passivated |
| Other Testing | NACE MRO175, Hardness Test, Flare, Hydrostatic Test, Eddy Current test, Grain Size Test, Eddy Current, Annealed, Tempered, Stress Relieved etc. |
| Dimension | All Pipes Is Manufactured and Inspected / Tested to the Relevant standards including ASTM And ASME |
Equivalent Grade:
| STANDARD | UNS | WERKSTOFF NR. | OR | BS | JIS | AFNOR | GOST | EN |
| Incoloy 800 | N08800 | 1.4876 | XH32T | NA 15 | NCF 800 | Z8NC32-21 | ЭИ670 | X10NiCrAlTi32-20 |
Chemical Composition%:
| Ni | Cr | Fe | Ti | Al | C | Mn | Si | S | Cu |
| 30.0-35.0 | 19.0-23.0 | ≥39.5 | 0.15-0.60 | 0.15-0.60 | ≤0.10 | ≤1.50 | ≤1.00 | ≤0.015 | ≤0.75 |
Mechanical Properties:
| Grade | ASTM B407 Incoloy 800 |
| Tensile Strength (MPa) min | 520 MPa |
| Yield Strength 0.2% Proof (MPa) min | 205 MPa |
| Elongation (% in 50mm) min | 30% |
Why Choose Gnee Nickel Alloy (Supplier Example)?
✅ Large stock of Incoloy 800/800H/800HT alloy tubes/bars/plates/fittings, fast shipping.
✅ Factory direct sales, highly competitive prices, excellent value for money.
✅ Comprehensive quality assurance: Material Testing Certificate (MTC), chemical composition certificate, and mechanical properties certificate.
✅ Value-added services: slitting, cutting, polishing, surface treatment.
✅ Worldwide shipping, secure and reliable packaging, and provision of export-required documents.
Email: ss@gneesteel.com
Gnee Steel is a supplier of Incoloy 800/800H/800HT steel, offering a wide range of products including: seamless pipe (sizes: 4-219 mm; thickness: 0.5-20 mm); welded pipe (sizes: 5.0-1219.2 mm; thickness: 0.5-20 mm); plates (thickness 0.1 to 100 mm; width 10-2500 mm); strips; alloy round bars (diameter 3-800 mm); flat bars (thickness 2-100 mm; width 10-500 mm); hexagonal bars (size 2-100 mm); wire rods; and extruded profiles. We collaborate with steel mills to provide our customers with 800 series alloys, meeting or exceeding numerous leading industry standards, including ASTM, ASME, SAE, AMS, ISO, DIN, EN, and BS standards.
Gnee Steel stocks and sells Incoloy 800/800H/800HT steel, including pipes, plates, strips, round bars, flat bars, forged billets, hexagonal steel, wire rods, and extruded profiles. Please feel free to contact us at ss@gneesteel.com for a quote.