Aug 11, 2025 Leave a message

Datasheet-For-Inconel-600-1-7-(1)-1-6.pdf

About Inconel 600 Seamless Pipe

 
 
 
Information about Inconel 600 seamless pipe
01.

About Inconel 600 Seamless Pipe

Inconel 600 seamless pipe is a nickel-chromium alloy pipe known for its excellent resistance to high temperatures, corrosion, and oxidation. It's a versatile material used in various industries, including aerospace, chemical processing, and nuclear engineering, due to its ability to withstand extreme environments.

02.

What is Inconel 600 used for?

Inconel 600 is a nickel-chromium alloy widely used in high-temperature and corrosive environments due to its excellent oxidation resistance, strength, and resistance to various corrosive substances. Its applications include aerospace, chemical processing, heat treatment, and nuclear power generation.

Inconel 600

Inconel Alloy 600 Pipe Specification

Category Details
ASTM Specification ASTM B 167 ASME SB 167 / ASTM B 829 ASME SB 829 / ASTM B 517 ASME SB 517
Standard ASTM, ASME, JIS, AISI, AMS, EN, SAE, DIN, NF, TOCT, DS, DTD, GB
ASTM B167 Inconel 600 Seamless Pipe Size 4 to 219mm W. T.: 0.5 to 20mm
Swg & Bwg 12 Swg., 10 Swg., 16 Swg., 14 Swg., 20 Swg., 18 Swg.
600 Inconel Pipe Schedule XS, SCH30, SCH40, XXS, SCH80, SCH120, SCH60, SCH140, STD, SCH10, SCH10S, SCH40S, SCH80, SCH20, SCH5, SCH160
Inconel 600 Pipe Length Double Random, Single Random, Standard & Cut length Pipe
Finish Polished, AP (Annealed & Pickled), BA (Bright & Annealed), MF, NO.1, NO.4, 2B, BA, HL, 8K, Mirror finish, etc
Type of 600 Alloy Pipe Seamless
Inconel 600 Pipe End Plain End, Beveled End, Threaded Pipe, Screwed ends

Chemical Composition of Inconel 600 Pipe

 

Element Carbon (C) Manganese (Mn) Silicon (Si) Iron (Fe) Sulfur (S) Chromium (Cr) Copper (Cu) Nickel (Ni)
Min (%) – – – 6.0 – 14.0 – 72.0
Max (%) 0.15 1.0 0.5 10.0 0.015 17.0 0.5 –

Mechanical Properties of Inconel 600 Seamless Pipes

 

Grade Tensile Strength Yield Strength (0.2% Proof) Elongation (% in 50mm) Hardness
Inconel 600 Pipe Psi: 95,000 (min) / MPa: 655 (min) Psi: 45,000 (min) / MPa: 310 (min) 40 (min) Rockwell B (HR B): – (max)
Brinell (HB): – (max)
Gnee Steel

 

About Gnee Steel

Gnee Steel specializes in the production and sale of various nickel-based alloys, including Nickel 201, Nickel 202, Hastelloy C-276, Hastelloy C-22, Hastelloy B, Hastelloy C-4, Inconel Alloy 600, Inconel 625, Inconel 718, Inconel X-750, Incoloy Alloy 800, Incoloy 800H/HT, Incoloy 825, Monel Alloy 400, Monel K500, and high-temperature alloys. Gnee Steel's products are widely used in aerospace, chemical, electric power, automotive, and nuclear energy applications. We also offer customized alloy solutions tailored to customer needs. For alloy pricing inquiries or customized alloy solutions, please contact us for a quote at ss@gneesteel.com.

Send Inquiry