What is the difference between Inconel 600 and SS 304?
Inconel 600 and SS 304 are two distinct metal alloys with distinct properties and uses. Inconel 600 is a nickel-chromium alloy known for its excellent high-temperature strength and corrosion resistance, particularly in harsh environments such as the aerospace and nuclear industries. SS 304, a stainless steel with good corrosion resistance, is widely used in a variety of applications due to its cost-effectiveness and ease of fabrication.
What are the standard Inconel 600 pipes?
These pipes conform to ASTM B167, B829, and B517 specifications. Pipes are available in various sizes according to ASTM, ASME, and API standards. Inconel 600 seamless pipes are available in diameters from 4 mm to 219 mm, while welded and EFW pipes are available in diameters from 5 mm to 1219.2 mm, with wall thicknesses ranging from 0.5 mm to 20 mm.

Inconel 600:
Composition: Primarily nickel and chromium, with a small amount of iron.
High-Temperature Performance: Excellent strength and resistance to oxidation and scaling at high temperatures.
Corrosion Resistance: Excellent resistance to a wide range of corrosive media, including chloride stress corrosion cracking.
SS 304:
Composition: Primarily iron, with some chromium and nickel.
High-Temperature Performance: Limited strength and oxidation resistance at high temperatures.
Corrosion Resistance: Good corrosion resistance, suitable for a variety of applications.
Summary of the main differences between Inconel 600 and SS 304:
|
Feature |
Inconel 600 |
SS 304 |
|---|---|---|
|
High-Temperature Strength |
Excellent |
Limited |
|
Corrosion Resistance (General) |
Excellent |
Good |
|
Fabrication |
Difficult |
Easy |
|
Cost |
High |
Low |
|
Primary Use Cases |
Aerospace, nuclear |
General industrial, food processing |

Gnee Steel is a supplier of Inconel 600 and SS 304, offering a wide range of products including seamless pipes (sizes from 4 to 219 mm, thicknesses from 0.5 to 20 mm), welded pipes (sizes from 5.0 to 1219.2 mm, thicknesses from 0.5 to 20 mm), plates (thicknesses from 0.1 to 100 mm, widths from 10 to 2500 mm), strip, alloy round bars (diameters from 3 to 800 mm), flat bars (thicknesses from 2 to 100 mm, widths from 10 to 500 mm), hexagonal bars (2 to 100 mm), wire rod, and extruded sections. We partner with steel mills to provide our customers with 625 alloy that meets or exceeds numerous leading industry standards, including ASTM, ASME, SAE, AMS, ISO, DIN, EN, and BS. Gnee Steel stocks and sells Inconel 600 and SS 304, pipe, tube, plate, strip, sheet, round bar, flat bar, forging billet, hexagon, wire and extruded sections. Feel free to contact us for a quote at ss@gneesteel.com