Inconel 600 Seamless Pipe
video

Inconel 600 Seamless Pipe

Inconel 600 seamless pipes
Sizes: 4 - 219 mm
Thickness: 0.5 - 20 mm
Lengths: single, double, random and cut to length

As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.

Product Introduction

Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of inconel 600 seamless pipe in China. If you're going to wholesale high quality inconel 600 seamless pipe made in China, welcome to get free sample from our factory. Good service and reasonable price are available.

 

Ni 600 Seamless Pipe Description

Nicke Alloy 600 Seamless Pipe

 

Gnee Steel Nicke Alloy 600 Seamless Pipe

Inconel 600 pipes are used for high temperature applications up to 2000F as well as cryogenic applications. The material has good weldability and strong corrosion resistance. The material has high resistance to carburization and oxidation. Gnee Steel is one of the leading manufacturers and a leading supplier of Inconel 600 pipe products.
These pipes meet ASTM B167, B829 and B517 specifications. There are different sizes as per ASTM, ASME and API standards. Inconel 600 pipes range from 4mm to 219mm (seamless pipes), 5 to 1219.2mm (welded and EFW pipes) with wall thickness ranging from 0.5mm to 20mm. Alloy 600 seamless pipes are produced using cold rolling process with less absolute roughness and high dimensional accuracy. These pipes are suitable for instrumentation applications. These pipes are dedicated for large diameter pipes.

Inconel 600 Seamless Pipe Sizes In Mm

WT= wall thickness, OD= Outside Diameter, ID= Inside Diameter

Inconel 600 Pipe OD
mm
Pipe WT
mm
in. Sch Kg/m
13.72 1.65 1/4 10S 0.50
13.72 2.24 1/4 40S 0.64
13.72 3.02 1/4 80S 0.81
17.15 1.65 3/8 10S 0.64
17.15 2.31 3/8 40S 0.86
17.15 3.20 3/8 80S 1.12
21.34 2.11 1/2 10S 1.02
21.34 2.77 1/2 40S 1.29
21.34 3.73 1/2 80S 1.65
26.67 2.11 3/4 10S 1.30
26.67 2.87 3/4 40S 1.71
26.67 3.91 3/4 80S 2.23
33.40 2.77 1 10S 2.13
33.40 3.38 1 40S 2.54
33.40 4.55 1 80S 3.29
33.40 6.352) 1 160 4.30

Nickel Alloy 600 Seamless Pipe Specifications

Trade name Inconel Alloy 600 Seamless Pipe
Alloy 600 Pipes Standard AISI, DIN, EN, GB, JIS, ASTM, ASME
Inconel 600 Seamless Pipe Dimensions ANSI/ASME B36.19, B36.10
Pipe Schedule SCH 5, SCH10, SCH 40, SCH 80, SCH 80S, SCH 160, SCH XXS, SCH XS
Form Round
Length Single Random, Double Random, Standard & Cut length
End Plain End, Beveled End, Treaded.

Inconel Tube

N06600 Tubing Chemical Composition

Grade C Mn Si S Cu Fe Ni Cr
Inconel 600 0.15 max 1.00 max 0.50 max 0.015max 0.50 max 6.00 – 10.00 72.00 min 14.00 – 17.00

Nickel Alloy 600 Tubes Mechanical Properties

Element Density Melting Point Tensile Strength Yield Strength (0.2%Offset) Elongation
Inconel 600 8.47 g/cm3 1413 °C (2580 °F) Psi – 95,000 , MPa – 655 Psi – 45,000 , MPa – 310 40 %

Inconel 600 Seamless Pipe Features and Applications

Inconel 600 Seamless Pipe Features

Resistant to a wide range of corrosive media.

Virtually immune to chlorine ion stress corrosion cracking

Non-magnetic

Excellent mechanical properties

Alloy 600 Seamless Pipe Applications

Industry Application
Petrochemical & Refining

Steam lines, alkylation units, flare systems, and reboilers handling acidic fluids

Nuclear & Power Plants

Steam generator tubing, reactor cores, control rod components, and heat shields

Heat Treatment Equipment

Furnace muffles, radiant tubes, and thermocouple protection sheaths

Chemical Processing

Process piping for acids, alkalis, oxidizers, and solvents

Aerospace

Jet engine components, turbine exhaust systems, and afterburner liners

Marine Engineering

Seawater piping, condenser tubes, and heat exchangers exposed to chloride ions

Food & Beverage Industry

Steam and hot water lines requiring sanitation and corrosion resistance

Electronics & Instrumentation

Thermocouple sheaths and sensor tubing in corrosive environments

Ni 600 Pipe Testing And Qualification Certificate

Alloy 600 Pipe Testing And Qualification Certificate

Alloy 600 Pipe Testing
Alloy 600 Pipe Testing
Alloy 600 Pipe Qualification Certificate
Alloy 600 Pipe Qualification Certificate

About Gnee Steel

Gnee Steel

 

About Gnee Steel

Gnee Steel is a supplier of Inconel 600 Seamless Pipe, with products covering pipes: Seamless pipes: Size: 4 - 219 mm; Thickness: 0.5 - 20 mm; Welded pipes: Size: 5.0 - 1219.2 mm; Thickness: 0.5 - 20 mm, Plates: Plate thickness 0.1 to 100 mm; Plate width 10-2500 mm, Strips, Alloy round bar sizes: diameter 3-800 mm;, Flat bar sizes: thickness 2-100 mm; Width: 10-500 mm, Hexagonal bar sizes: 2-100 mm;, Wire and extruded profiles. We work with steel mills to provide customers with 625 alloy, and its products meet or exceed many leading industry standards, including ASTM, ASME, SAE, AMS, ISO, DIN, EN and BS standards.
Gnee Steel stocks and sells Inconel 600 Seamless Pipe, Tubes, Pipes, Plates, Strips, Plates, Round Bars, Flat Bars, Forged Billets, Hexagons, Wires and Extruded Profiles. Feel free to contact us for a quote at ss@gneesteel.com

Hot Tags: inconel 600 seamless pipe, China inconel 600 seamless pipe suppliers, Duplex Stainless Steel, inconel tube, nickel iron based alloy, inconel alloy ss tubing, Hastelloy B, hastelloy material piping alloy