Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of monel slip on flanges in China. If you're going to wholesale high quality monel slip on flanges made in China, welcome to get free sample from our factory. Good service and reasonable price are available.
Monel Slip On Flanges
Product Introduction
Monel Slip On Flanges offer outstanding characteristics as they provide exceptional resistance to hydrofluoric acid. Particularly with the tough acid to deal with, in all concentrations up to the boiling point. Monel Slip On Flanges is perhaps the most resistant of all commonly used specialty products for hydrofluoric acid applications.Monel is a nickel-based alloy; hence it offers good mechanical properties such as high tensile strength, elongations, yield strength.
SPECIFICATION OF MONEL SLIP ON FLANGES
| Specifications | ASTM B564 / ASME SB564 |
| Size | 1/2″ (15 NB) to 48″ (1200NB) DN10~DN5000 |
| Dimensions | ANSI/ASME B16.5, B16.47 Series A & B, B16.48, BS4504, BS 10, EN-1092, DIN, ANSI Flanges, ASME Flanges, BS Flanges, DIN Flanges, EN Flanges, GOST Flange, ASME/ANSI B16.5/16.36/16.47A/16.47B, MSS SP44, ISO70051, JISB2220, BS1560-3.1, API7S-15, API7S-43, API605, EN1092 |
| Pressure Rating | Class 150 LBS, 300 LBS, 600 LBS, 900 LBS, 1500 LBS, 2500 LBS |
| Connect Type/ Flange Face Type | Raised Face (RF), Ring Type Joint (RTJ), Flat Face (FF), Large Male-Female (LMF), Lap-Joint Face (LJF), Small Male-Female (SMF), Small Tongue, Large Tongue & Groove, Groove |