Monel 400 Alloy Coil
video

Monel 400 Alloy Coil

Specifications
Form: Slit roll, gasket roll or regular roll
Width: 0.5 to 1.2m
Thickness: 0.1mm to 5.0mm
Standard: ASME SB127 and ASTM B127
Send Inquiry
Chat Now

As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.

Product Introduction

Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of monel 400 alloy coil in China. If you're going to wholesale high quality monel 400 alloy coil made in China, welcome to get free sample from our factory. Good service and reasonable price are available.

 

Monel metal 400 Coil introduce

metal 400 Alloy Coil

Monel 400 Alloy CoilMonel 400 Alloy Coil

Introduction to Monel 400 Steel Coils:

Monel 400 Coil is an alloy that consists mainly of nickel and copper. That is why they are also known as Alloy 400 Coil. These coils also have elements like cobalt and sulfur added to them. Typically, Alloy 400 Coil is used in exhaust applications, furnaces, hot water tanks, hydraulic lines, pressure vessels, chemical equipment, and other applications and industries.

Alloy 400 Coils are well suited for these applications due to their high durability, excellent mechanical properties, corrosion resistance, and good weldability. In addition, they are resistant to alkaline atmospheres, high temperatures, non-oxidizing chlorides, hydrofluoric acid, and hydrochloric acid.

There are two techniques for producing Monel Alloy 400 Coils: cold rolling and hot rolling. They are produced by rolling or flattening Monel Alloy 400 plates or sheets.

Gnee Steel offers hot and cold rolled Monel 400 Coils in a variety of lengths, thicknesses, and other configurations to meet any project needs. To meet your specific needs, we can also customize to your exact requirements.

Key Features:

Corrosion Resistance: Seawater, acids, and alkalies are only a few of the corrosive conditions that Monel 400 steel coils exhibit exceptional resistance to. For applications where exposure to corrosive elements is unavoidable, such as maritime, chemical processing, and offshore, this makes them especially well-suited.
Mechanical Strength: Monel 400 has remarkable mechanical qualities, including as high strength and exceptional ductility, even in the face of corrosion. Because of these qualities, it may be used for equipment and structural parts that are subjected to significant mechanical loads and stress.
Temperature Stability: Across a broad temperature range, from cryogenic to high, Monel 400 has strong mechanical qualities and stability. Because of its adaptability, it may be used in a variety of settings, such as aerospace, where temperature swings are typical.

Applications:

 

Marine Engineering: Monel 400 steel coils find extensive use in marine engineering applications, including seawater piping systems, heat exchangers, and marine fittings. Its corrosion resistance and mechanical strength make it an ideal choice for components exposed to corrosive seawater environments.

Chemical Processing: In chemical processing industries, Monel 400 is utilized in reactors, vessels, and pumps handling corrosive chemicals. Its resistance to acids and alkalis makes it suitable for a wide range of chemical processing applications.

Aerospace: Monel 400's high strength-to-weight ratio and temperature stability make it suitable for aerospace applications, including aircraft components and structural parts where reliability and performance are critical.

Oil and Gas: Monel 400 steel coils are used in the oil and gas industry for downhole equipment, valves, and tubing systems. Its corrosion resistance and mechanical properties make it well-suited for offshore and subsea applications.

Standard Specification For Monel 400 Coils

Specifications : ASTM B127 / ASME SB127

Dimensions : ASTM, ASME, and API

Width : 1000mm, 1219mm, 1500mm, 1800mm, 2000mm, 2500mm, 3000mm, 3500mm, etc

Thickness : 4mm-100mm

Length : 2000mm, 2440mm, 3000mm, 5800mm, 6000mm, etc

Surface Finish : 2B, 2D, BA, NO.1, NO.4, NO.8, 8K, hairline, sand blast, Brush, etching, Hot rolled coils (HR), Cold rolled Coils (CR), SATIN (Met with Plastic Coated) etc

Hardness : Soft, Hard, Half Hard, Quarter Hard, Spring Hard etc.

Form : Coils, Foils, Rolls, Plain Coils, Shim Coils, Strip, Flats, Blank (Circle), Ring (Flange) etc.

Monel 400 Coils Chemical Composition

Grade C Mn Si S Cu Ni Fe
Monel 400 0.30 max 2.00 max 0.50 max 0.024 max 28.0 - 34.0 63.0 min 2.50 max

Monel 400 Coils Mechanical Properties

Element Density Melting Point Tensile Strength Yield Strength (0.2%Offset) Elongation
Monel 400 8.8 g/cm3 1350 °C (2460 °F) Psi – 80,000 , MPa – 550 Psi – 35,000 , MPa – 240 40 %

GNEE Group Factory Environment

Monel metal 400 Alloy Coil

Monel 400 Alloy Coil


GNEE Group Product Packaging

Monel 400 Coil

Monel 400 Alloy Coil

FAQ

Q: What are the advantages of your company?
A: We have many professionals, technicians, more competitive prices and the best after-sales service than other stainless steel companies.
Q: How many countries have you exported to?
A: Exported to more than 50 countries, mainly from the United States, the United Kingdom, Kuwait, Egypt, Turkey, Jordan, India, etc.
Q: Can you provide samples?
Answer: Yes. As long as you contact us, we can provide free small samples in stock. Customized samples will take about 5-7 days.

Hot Tags: monel 400 alloy coil, China monel 400 alloy coil suppliers, alloy contract, alloy cost benefit analysis, alloy retailer, alloy accounting, alloy annealing, alloy competitor

Send Inquiry

whatsapp

Phone

E-mail

Inquiry