400 450 401 Monel Round Pipe
Racing car exhaust systems
Jet engine exhaust systems
Aerospace equipment
Chemical processing
Acid gas production tubes
Nuclear waste reprocessing equipment
Chimney linings
As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.
- Send E-mail: ss@gneesteel.com
Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of 400 450 401 monel round pipe in China. If you're going to wholesale high quality 400 450 401 monel round pipe made in China, welcome to get free sample from our factory. Good service and reasonable price are available.
400 450 401 Monel Pipe information
400 450 401 monel tube video
GNEE STEEL GROUP supplies 400 450 401 Monel Pipe for you
GNEE STEEL GROUP supplies 400 Monel Pipe
UNS N04400
Other common names: Alloy 400
W.Nr.2.4360, 2.4361
ASTM: B164, B564, B127, B165, B725, B730
ASME: SB164, SB564, SB127, SB165, SB725, SB730
QQ-N-281
Mil-T-1368
EN10204 3.1
|
Form |
Standard |
|---|---|
|
Metal Type |
UNS N04400 |
|
Bar |
ASTM B164 QQ-N-281 Din 17750 |
|
Wire |
|
|
Sheet |
ASTM B127 QQ-N-281 |
|
Plate |
ASTM B127 QQ-N-281 |
|
Pipe |
ASTM B165 |
|
Tube |
ASTM B165 |
|
Fitting |
|
|
Forging |
ASTM B564 |
|
Weld Wire |
FM 60/ ERNiCu-7/ 17753 |
|
Weld Electrode |
FM 190 ENiCu-7 |
|
Din |
2.4360 |
| PRODUCT FORM | SIZE RANGE FROM | SIZE RANGE TO |
|---|---|---|
| Alloy 400 round bar | 4.76 mm | 279 mm |
| Alloy 400 round tubing | 3.175 mm | 19.05 mm |
| Alloy 400 sheet & plate | 0.5 mm | 76.2 mm |
| Alloy 400 pipe | 0.25 in | 8 in |
| Alloy 400 pipe fittings | 0.25 in | 8 in |
| Alloy 400 flanges | 0.25 in | 8 in |
GNEE STEEL GROUP supplies 450 Monel Pipe:
Alloy 450
UNS N45000
GNEE is available in monel 450 product form:
hexagon
round
apartment
Forgings
tube
pipeline
plate
metallic line
sheet
GNEE STEEL GROUP supplies 401 Monel Pipe:
• Monel 401
• UNS N04401
• W.Nr. 2.0842
• DIN 17471
GNEE STEEL provides you with a variety of monel 401 product forms, including but not limited to:
• stick/rod
• Pipes/Tubes
• Coil/strip
• Plate/sheet/circle
• metallic line
• Pipe fittings (flanges, elbows, tees...)
• custom made
400 450 401 Monel Pipe Specification
monel 400 Tubing chemical composition
| Element | Content (%) |
|---|---|
| Nickel, Ni | 63-70 |
| Copper, Cu | 28-34 |
| Iron, Fe | 2.5 |
| Manganese, Mn | 2 |
| Silicon, Si | 0.5 |
| Carbon, C | 0.3 |
| Sulfur, S | 0.024 |
|
The Chemical Composition of Alloy 450/ Monel 450, % |
|
|---|---|
| Ni | 29.0-33.0 |
| Cu | Balance |
| Fe | 0.4-1.0 |
| Mn | ≤1.0 |
| S | ≤0.020 |
| Zn | ≤1.0 |
| Pb | ≤0.05 |
| P | ≤0.020 |
Monel 401 Alloy Piping chemical composition
| Element | Content (%) |
|---|---|
| Nickel, Ni | 40 – 45 max |
| Copper, Cu | Remainder |
| Manganese, Mn | 2.25 max |
| Iron, Fe | 0.75 max |
| Silicon, Si | 0.25 max |
| Cobalt, Co | 0.25 max |
| Carbon, C | 0.10 max |
| Sulfur, S | 0.015 max |


Monel 400 alloy (UNS N04400 or MCu-28-1.5-1.8 or Ni68Cu28Fe) is a nickel-based alloy material. It has excellent corrosion resistance in seawater, chemical solvents, ammonia sulfur chloride, hydrogen chloride, and acidic media such as sulfuric acid, hydrofluoric acid, hydrochloric acid, phosphoric acid, and organic acids, as well as alkaline media, salts, and molten salts.
Monel 450 alloy, also known as nickel-copper alloy 450, is an alloy with good corrosion resistance and high strength. Its main components are about 70% nickel and 30% copper, while also containing small amounts of iron, manganese, silicon and other elements. Monel 450 alloy has excellent corrosion resistance, especially to salt water and acidic environments.
Monel 401 Alloy Properties Monel 401 is an alloy with a very low temperature coefficient of resistance and medium-range resistivity. It is mainly used in professional electrical and electronic applications.
GNEE Group Factory Environment
Alloy 400 450 401 Monel Round Pipe

400 450 401 Monel Pipe material & size
400 450 401 Monel Pipe material & size


customer visi
customer visit

FAQ
Q: Do you provide samples? Is it free or extra?
A: Yes, we can provide samples for free without paying the shipping cost.
Q: What are your payment terms?
A: Payment <=1000USD, 50% in advance. Payment >=1000USD, 30% T/T in advance, balance before shipment. or negotiable
Q: About the product price of 400 450 401 monel seamless pipe?
A: Due to cyclical changes in raw material prices, prices vary in different periods.
contact us
Address
No.4-1114 Beichen Building, Beicang Town, Beicheng District, Tianjin City, China
Phone
+86-15824687445
ss@gneesteel.com
Skype
mmkelly1314
Whatsapp/Wechat
+86 15824687445
Hot Tags: 400 450 401 Monel Round Pipe, China 400 450 401 Monel Round Pipe suppliers, alloy rod, machinable alloy, alloy tender, alloy billets, alloy aging, melting point alloy
You Might Also Like
Send Inquiry