Monel 404 alloy is a single-phase solid solution Ni-Cu alloy that has good corrosion resistance in many media environments. It has good corrosion resistance from slightly oxidizing media environment to neutral environment to suitable reducing environment.
Send Inquiry
Chat Now

As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.

Product Introduction

Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of monel 404 505 piping in China. If you're going to wholesale high quality monel 404 505 piping made in China, welcome to get free sample from our factory. Good service and reasonable price are available.

 

Monel 404 505 Piping information

monel 404 505 seamless piping video

GNEE STEEL GROUP supplies Monel 404 505 Piping for you

 

GNEE STEEL GROUP supplies Monel 404 Piping

UNS N04400

Other common names: Alloy 400

W.Nr.2.4360, 2.4361

ASTM: B164, B564, B127, B165, B725, B730

ASME: SB164, SB564, SB127, SB165, SB725, SB730

QQ-N-281

Mil-T-1368

EN10204 3.1

What forms of Monel 400 does GNEE STEEL offer?

Sheet

Plate

Bar

Pipe & Tube (welded & seamless)

Fittings

Elbows, tees, stub-ends, returns, caps, crosses, reducers, pipe nipples. etc.

Wire

 

Standard

AISI, ASTM, BS, DIN, GB, JIS

Grade

Monel series: 400 K500
Inconel series: 600 601 625 718 725
Incoloy series: 800 800H 825 925
Hastelloy series: B,B2,B3,C,C-276,C-4,C-22
Pure: Ni200, Ni201 

 

GNEE STEEL GROUP supplies Monel 505 Piping

What forms of Monel 505 does GNEE offer?
sheet
plate
bar
Pipes and Tubes (Welded and Seamless)
Accessories
Elbows, tees, short pipe ends, return pipes, pipe caps, crosses, reducers, pipe joints. ETC.
metallic line 

Monel 404 505 Piping chemical composition

Monel 404 Piping chemical composition

Element Content (%)
Nickel, Ni Remainder
Copper, Cu 28-34
Iron, Fe 2.5 max
Manganese, Mn 2 max
Silicon, Si 0.5 max
Carbon, C 0.3 max
Sulphur, S 0.024

 Monel 505 Piping chemical composition

Designation Cu % Al % Ti % Fe % Mn % Si % Ni %
Monel 505 28-34 - - 2.5 max. 2.0 max. 0.5 max. 63 min.

monel 404 505 piping

monel 404 505 ss piping suppliersmonel 404 505 alloy piping dealer

Monel 404 alloy is a single-phase solid solution Ni-Cu alloy that has good corrosion resistance in many media environments. It has good corrosion resistance from slightly oxidizing media environment to neutral environment to suitable reducing environment. This alloy has a long history of use as a corrosion-resistant material.
Monel 505 (NCu-30-4-2-1/Ni66Cu28Si4) high silicon Monel alloy is a Ni-Cu-Si-Fe-Mn series dispersion-strengthened nickel-copper alloy, also known as NCu-30-4-2-1. The silicon content is as high as more than 4%. The addition of silicon increases the strength, hardness and recrystallization temperature of the alloy, and improves the casting performance of the alloy. The adoption of new processes greatly refines the structure, eliminates component segregation and inclusions, and improves the mechanical properties of the material. Greatly improve.

 

Monel 404 505 Piping material & size

Monel 404 505 Piping material & size

Monel 404 505 Piping

Monel 404 505 Piping

 

customer visit

customer visit

Monel 404 505 Piping

 

FAQ

Q: Can you provide samples?
Answer: Yes. As long as you contact us, we can provide free small samples in stock. Customized samples will take about 5-7 days.

Q: Can you send samples?
A: Of course, we can send samples to all over the world, our samples are free, but customers need to bear the express cost.

Q: About the product price of monel 404 505 piping?
A: Due to cyclical changes in raw material prices, prices vary in different periods.

contact us

Address

No.4-1114 Beichen Building, Beicang Town, Beicheng District, Tianjin City, China

 

Phone

+86-15824687445

 

Email

ss@gneesteel.com

 

Skype

mmkelly1314

 

Whatsapp/Wechat

+86 15824687445

Hot Tags: monel 404 505 piping, China monel 404 505 piping suppliers, machinable alloy, alloy terms and conditions, alloy technology, alloy experience, alloy exporter, alloy hardening

Send Inquiry

whatsapp

Phone

E-mail

Inquiry