Monel K500 thick Plate
Standard: ASTM B127 / ASME SB127
Size: 1000mm x 2000mm, 1220mm x 2440mm, 1500mm x 3000mm, 2000mm x 2000mm, 2000mm x 4000mm
Form: Coil, Foil, Coil, Plain Sheet, Strip, Flat, Blank (Round), Ring (Flange), etc.
Hardness: Soft, Hard, Half Hard, Quarter Hard, Spring Hard, etc.
Thickness: 0.1mm to 12mm Thick
Length: 500mm to 12000mm
Width: 100mm to 3000mm
As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.
- Send E-mail: ss@gneesteel.com
Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of monel k500 thick plate in China. If you're going to wholesale high quality monel k500 thick plate made in China, welcome to get free sample from our factory. Good service and reasonable price are available.
Monel K500 thick Plate introduce
Monel K500 metal thick Plate


Monel K500 Sheet is made of a nickel-copper alloy that contains at least 63% nickel and 28% copper, along with carbon, manganese, silicon, sulfur and iron. Navstar Steel is a leading manufacturer and supplier of Monel K500 Sheet products in different sizes and types. It is available in thicker sheets and thinner sheets as well as coils and strips. The material has a very high melting point of 1350 degrees Celsius, making it suitable for high temperature applications. Monel K500 Sheet also has high tensile and yield strengths and high density.
Due to its unique properties, Monel K500 is widely used in applications where both high strength and resistance to corrosive environments are essential. Common applications include:
Marine engineering: Components like propeller shafts, pump shafts, and seawater handling equipment.
Oil and gas industry: Non-magnetic applications such as oil well tools and drill collars.
Chemical processing: Pumps, valves, and other equipment that encounter corrosive chemicals.
Aerospace: Fasteners and other high-stress components.
Chemical Composition Of Monel K500 Plates
| Grade | C | Mn | Si | S | Cu | Fe | Ni |
|---|---|---|---|---|---|---|---|
| Monel K500 | 0.25 max | 1.5 max | 0.5 max | 0.010 max | 27.00 – 33.00 | 0.5 – 2 | 63.00 min |
Monel K500 Plates, Sheets & Coils Mechanical Properties
| Element | Density | Melting Point | Tensile Strength | Yield Strength (0.2%Offset) | Elongation |
|---|---|---|---|---|---|
| Monel K500 | 8.44 g/cm3 | 1350 °C (2460 °F) | Psi – 160000 , MPa – 1100 | Psi – 115000 , MPa – 790 | 20 % |
GNEE Group Factory Environment
K500 Alloy thick Plate

GNEE Company Environment
Monel K500 Plate

FAQ
Q: What are the advantages of your company?
A: We have many professionals, technicians, more competitive prices and the best after-sales service than other stainless steel companies.
Q: How many countries have you exported to?
A: Exported to more than 50 countries, mainly from the United States, the United Kingdom, Kuwait, Egypt, Turkey, Jordan, India, etc.
Q: Can you provide samples?
Answer: Yes. As long as you contact us, we can provide free small samples in stock. Customized samples will take about 5-7 days.
Hot Tags: Monel K500 thick Plate, China Monel K500 thick Plate suppliers, alloy accounting, alloy usage, alloy optimization, sulfide resistant alloy, surface finish alloy, alloy risk