15-7Mo 654SMO Ss Pipe
PH 15-7 Mo is a precipitation-hardened stainless steel used in applications requiring high strength and moderate corrosion resistance. Similar to 17-7, 2% molybdenum is used in place of 2% chromium, giving 15-7 Mo greater room and temperature strength.
Send Inquiry
Chat Now
As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.
- Send E-mail: ss@gneesteel.com
Product Introduction
Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of 15-7mo 654smo ss pipe in China. If you're going to wholesale high quality 15-7mo 654smo ss pipe made in China, welcome to get free sample from our factory. Good service and reasonable price are available.
15-7Mo 654SMO Ss Pipe
15-7Mo 654SMO Ss Pipe Specification
| Element | Content (%) |
|---|---|
| Iron, Fe | Balance |
| Chromium, Cr | 14 -16 |
| Nickel, Ni | 6.50 - 7.75 |
| Molybdenum, Mb | 2 - 3 |
| Silicon, Si | 1 |
| Manganese, Mn | 1 |
| Aluminum, Al | 0.75 - 1.50 |
| Carbon, C | 0.09 |
| Phosphorus, P | 0.040 |
| Sulfur, S | 0.040 |
Hot Tags: 15-7mo 654smo ss pipe, China 15-7mo 654smo ss pipe suppliers, alloy wholesaler, alloy advantage, oil and gas alloy, alloy payment, alloy raw material, alloy compositions