Monel Alloy R405 Fasteners
video

Monel Alloy R405 Fasteners

Monel R405 Fasteners are forged fasteners made of copper-nickel alloy, titanium, and aluminum. These materials are extremely corrosion-resistant and possess high tensile strength.MONEL R405 is a nickel-copper alloy that has good corrosion resistance in most chemical environments. It is resistant to oxidizing acids, seawater, and steam at high temperatures. It also has good resistance to chloride-ion stress corrosion cracking. It is not recommended for welding.
Send Inquiry
Chat Now

As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.

Product Introduction

Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of monel alloy r405 fasteners in China. If you're going to wholesale high quality monel alloy r405 fasteners made in China, welcome to get free sample from our factory. Good service and reasonable price are available.

 

Product Introduction

 

Monel R405 Fasteners are fabricated using the same procedures as Monel 400. These fasteners are primarily used in screw machines. This metal is slightly magnetic at room temperature but can be hardened through cold work. It is a free-machining grade of Monel 400 and is primarily recommended for screw machines. Although it shares similar properties to Monel 400, Monel R-405 has increased sulfur content. As a result, it is more workable than Monel 400. Alloy R-405 is approved as a material of construction under Section VIII (Pressure Vessels - Division 1) of the ASME Boiler and Pressure Vessel Code and in Section III, Nuclear Vessels, of the Code.

 

MONEL alloy R-405 is fabricated, pickled and heat-treated by the same procedures as for alloy 400. The alloy is not recommended for forging.Monel R-405 Fasteners are designed for high-strength applications. Their high corrosion resistance makes them perfect for industrial and marine applications. 

 

Monel R405 Fasteners are resistant to corrosion, saltwater, and oxidizing media. They provide good protection against hydrofluoric acid, sulfuric acid, and hydrochloric acid. This makes them critical components for ships and offshore oil platforms.MONEL alloy R-405 was especially developed for good machinability and is recommended for use with automatic screw machines. The nickel-copper sulfides resulting from the sulfur in its composition act as chip breakers. Because of these inclusions the surface finish of the alloy is not as smooth as that of MONEL alloy 400.

 

product-1010-304

 

MONEL R405 FASTENER SPECIFICATION

Specifications ASTM B164 / ASME SB164, ASTM F467 / F468, ASME SF467 / SF468
Dimensions DIN 931, 933, 934, 7991, 976, 125, ASME B18.2.1, B18.3
Size Bolt / Screw Size : M3 – M56 | 3/6″ to 2″ | Custom Sizes Nuts Size : M3 – M56 | 3/6″ to 2″ | Custom Sizes Washers Size : M3 – M56 | 3/6″ to 2″ | Custom Sizes Machine Screws Size : M1.6 – M12 Self Tapping Screw Size : No.2 – No. 14
Length 3 mm to 200 mm
Threads UNF, BSW, BSF, METRIC, UNC, or as required
Surface Coating Ptfe Coating Phosphate Coating Teflon Coating Zinc Coating Hot Dipped Galvanizing Coating Cadmium Coating Xylon Coating

 

product-1034-419

product-1028-338

 

 

MONEL R405 FASTENERS CHEMICAL COMPOSITION

Grade Ni Fe C Mn Si Cu Al S
Monel R405 63 min 2.5 max 0.3 max 2.0 max 0.5 max 28.0-34.0 – 0.025 – 0.060

 

MECHANICAL PROPERTIES OF MONEL R405 FASTENERS

Properties Metric Imperial
Density 8.8 gm/cm3 0.318 lb/in3

 

product-1075-406

Hot Tags: monel alloy r405 fasteners, China monel alloy r405 fasteners suppliers, alloy research, alloy inspection, alloy duty, alloy forging, alloy customer satisfaction, alloy surplus

Send Inquiry

whatsapp

Phone

E-mail

Inquiry