Monel Alloy K500 Buttweld Fittings
video

Monel Alloy K500 Buttweld Fittings

Monel 400/K500 is a Nickel-Copper alloy that offers excellent resistance and great strength. These alloys offers excellent resistance to many corrosive environment such as seawater, sulphuric acid, hydrofluoric acid, and alkalis.
Send Inquiry
Chat Now

As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.

Product Introduction

Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of monel alloy k500 buttweld fittings in China. If you're going to wholesale high quality monel alloy k500 buttweld fittings made in China, welcome to get free sample from our factory. Good service and reasonable price are available.

 

What is Monel Alloy K500 Buttweld Fittings

 

We, Gnee Steel Group, are a well-known supplier, manufacturer, and exporter of Monel K500 Buttweld Fittings. We provide these fittings. These Fittings are designed as per the international quality standards of raw materials.

Description & Composition Of Monel K500 Buttweld Fittings

Monel K500 is a solid-solution binary alloy. Monel alloy is a group of nickel alloys composed of nickel and copper elements with small amounts of iron, carbon, manganese, and silicon. In this, the alloys with copper contents 60% or more than that are called cupronickel. These alloy is stronger than a pure nickel. The nickel and copper are mutually soluble in all proportions that's why this alloy is a single-phase alloy. And, compared to steel, the Monel alloy is very difficult to machine.

 

The work-hardens of the alloy is quick. The alloy is needed to work at slow speeds and low feed rates. Usually, the alloy is used in applications that are in highly corrosive conditions. K500 is the first age hardenable nickel alloy. The huntington alloys are developing a new kind of Monel alloy by adding other elements to its chemistry for its increased strength. K500 increased properties by adding aluminum and titanium to the nickel-copper base alloy. It is going to heat under controlled conditions. It has thermal processing used to effect precipitation, usually known as age hardening or aging.

The Buttweld Fitting is a weldable fitting that allows to change the flow of direction, branch off, reduce pipe size. Buttweld fittings use a seamless or welded pipe as a starting material and are formed through multiple processes.

 

product-963-247

 

Properties And Application Monel K500 Buttweld Fittings

It has excellent features like being dimensionally stable, durable, rustproof, and more. The Monel alloy is resistant to corrosion by many agents, which are including rapidly flowing seawater. It can be fabricated easily by hot and cold working, machining, and welding. It combines the excellent corrosion resistance property of Monel alloy with the added advantages of greater strength and hardness. The strength and hardness increase by the impact resistance. It is used in the application are as follows:

                                                                                 Oil and gas pipeline

                                                                                 Chemical industry

                                                                                 Plumbing

                                                                                 Heating

 

Specification of Monel K500 Buttweld Fittings

Specifications : ASTM B366/ ASME SB366

Size : ½"NB to 48"NB

Dimensions : ASME/ANSI B16.9, ASME B16.28, MSS-SP-43, BS4504, BS4504, BS1560, BS10

Types : Seamless / Welded / Fabricated

Thickness : SCH10, SCH20, SCH30, STD SCH40, SCH60, XS, SCH 80, SCH 100, SCH 120, SCH 140, SCH 160, XXS available with NACE MR 01-75

Bending Radius : R=1D, 2D, 3D, 5D, 6D, 8D, 10D or Custom

 

Monel K500 Buttweld Pipe Fittings Chemical Composition

Monel K500

Ni

Fe

C

Mn

Si

Cu

S

63 min

0.5-2

0.25 max

1.5 max

0.5 max

27-33

0.010 max

 

Monel K500 Buttweld Pipe Fittings Mechanical & Physical Properties

Density

Melting point

Tensile Strength

Yield Strngth

Elongation

8.44 g/cm3

2400-2460 Deg F

Psi – 160000,

Mpa – 1100

Psi – 115000,

Mpa – 790

20%

 

Monel Alloy K500 Butt weld Pipe Fittings Specification

Specifications ASTM B366 / ASME SB366

Dimensions ASME/ANSI B16.9, ASME B16.28, MSS-SP-43, MSS SP-79

Size Seamless 1/2" - 10" , Welded 1/2" - 48"

Type (Seamless & 100% X-Ray Welded, Fabricated)

Bending Radius R=1D, 2D, 3D, 5D, 6D, 8D, 10D or Custom

Thickness Sch 5s, Sch 10s, Sch 40s, Sch 80s, Sch 160s, Sch XXS

Grade Monel K500 Pipe Fittings UNS (N05500), DIN (2.4375)

 