Monel Alloy 400 Stud Bolts
video

Monel Alloy 400 Stud Bolts

Specifications: ASTM F2281, ASTM B164/ASME SB164/SF2281
Standards: DIN, ASTM, BS and all international standards
Lengths: Up to 1 meter stud bolts
Sizes: M3 - M56 | 3/6" to 2" | Custom sizes
Heat treatment: Annealed, stress relieved, case hardened, quenched and tempered.
Send Inquiry
Chat Now

As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.

Product Introduction

Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of monel alloy 400 stud bolts in China. If you're going to wholesale high quality monel alloy 400 stud bolts made in China, welcome to get free sample from our factory. Good service and reasonable price are available.

 

Monel Alloy 400 Stud Bolts Introduction

metal Alloy 400 Stud Bolts

Monel Alloy 400 Stud BoltsMonel Alloy 400 Stud Bolts

Monel Alloy 400 Stud Bolts are a type of fastener made from a nickel-copper alloy that offers excellent strength and corrosion resistance compared to other metals or alloys. These bolts are machined from solid bar stock and are threaded at both ends for a secure connection.

The main use of Monel 400 stud bolts is to provide stability to components that require high tensile strength such as machine frames, pressure vessels, piping systems, valves, pumps, etc. In addition, since these stud bolts offer excellent resistance to saltwater environments or corrosive chemicals such as sulfuric acid, they can be used in applications that require maximum corrosion resistance. They also have excellent weldability, making them suitable for high-pressure projects such as boilers or pressure vessels. There is another grade of Monel stud bolts available, which is the Monel K500 stud bolts.

Monel 400 Stud Bolts

Monel Alloy 400 Stud Bolts

Monel 400 Stud bolts are unique from other stud bolts. Their creep fighting ability and capacity is commendable. Monel 400 Stud bolts exhibit superb tensile strength at higher temperatures. Operating conditions where greater performance features are required are fully satisfied by using this alloy. The molybdenum content of this alloy makes them tougher than stainless. Monel 400 Stud bolts are ready to bear attacks of acetic acids, sulphuric acid, citric and tartaric acids. Being low carbon austenitic alloy, they can stand strong against harsh media. Cold forming results in increasing its overall yield and strength. Monel 400 Stud bolts can work cognitively in marine atmospheres as well. The other industries used are the oil and gas industry, food processing industry, etc. The fabricability of Monel 400 Stud bolts is also appreciable. Their machinability is worth the recommendation. Continuous work has immunity to a good oxidation shield given by these alloys. Monel 400 Stud bolts support the welding process strongly as they eliminate the causing of carbide chromium precipitation.

 

The density of the material composition of these Stud bolts is higher than chromium. The density of the Monel 400 Stud bolts is 8.8 grams per centimetre cube. There are different mechanical and physical properties are offered by Monel 400 Stud bolts, and that's why they broadly used in different types of applications. They contain a great surface finish in different forms. We also manufacture the different types and forms of Monel 400 Stud bolts. They have got the best support from industrial applications as they work flexibly and reliably.

 

 

ASTM B164 MONEL 400 STUD BOLTS EQUIVALENT GRADES

Grade DIN UNS JIS BS GHOST AFNOR EN
Monel 400 2.4360 N04400 NW 4400 NA 13 МНЖМц 28-2,5-1,5 NU-30M NiCu30Fe

CHEMICAL COMPOSITION OF MONEL 400 STUD BOLTS

Grade C Mn Si Cu S Fe Ni
Monel 400 0.30 max 2.00 max 0.50 max 28.00 – 34.00 0.024 max 2.50 max 63.00 min

MECHANICAL PROPERTIES OF MONEL 400 FLANGES

Density Melting Point Tensile Strength Yield Strength (0.2%Offset) Elongation
8.8 g/cm3 1350 °C (2460 °F) Psi – 80,000 , MPa – 550 Psi – 35,000 , MPa – 240 40 %

GNEE Group Factory Environment

Alloy 400 Stud Bolts

Monel Alloy 400 Stud Bolts

GNEE Group Product Testing

Monel metal 400 Stud Bolts

Monel Alloy 400 Stud Bolts

FAQ

Q. What are your company's main products ?
A: Our main products are nickel-based alloys, Hastelloy, Inconel, Incoloy, Monel, stainless steel, carbon steel, galvanized steel, aluminum products, etc.
Q. How do you control quality ?
A: Mill Test Certification is supplied with shipment, Third Party Inspection is available. and we also get ISO,SGS Verified.
Q: What are the advantages of your company ?
A: We have many professionals, technical personnel, more competitive prices and best after-dales service than other stainless steel companies.

Hot Tags: monel alloy 400 stud bolts, China monel alloy 400 stud bolts suppliers, chemical industry alloy, dimensional stability alloy, alkali resistant alloy, alloy experience, nickel copper alloy, alloy bid

Send Inquiry

whatsapp

Phone

E-mail