Monel Alloy K500 corrosion resistant Pipes
video

Monel Alloy K500 corrosion resistant Pipes

Monel K500 Seamless Tube

Sizes (OD): .375" to 1" OD
Wall Thickness: .035" to .065" OD
Send Inquiry
Chat Now

As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.

Product Introduction

Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of monel alloy k500 corrosion resistant pipes in China. If you're going to wholesale high quality monel alloy k500 corrosion resistant pipes made in China, welcome to get free sample from our factory. Good service and reasonable price are available.

 

Monel Alloy K500 Pipes introduce

Alloy K500 corrosion resistant Pipes

Monel Alloy K500 corrosion resistant PipesMonel Alloy K500 corrosion resistant Pipes

Gnee Steel Group is a well-known supplier of our precipitation hardenable nickel copper alloy Monel K500 Pipe and Tubes. We have a team of skilled and professional people who advise and monitor the manufacturing process. We make pipes and tubes with a stable chemical composition of elements. We make good use of our cutting-edge technologies. The skilled team oversees the manufacturing process to produce a wide selection of Monel K500 Seamless Pipes & Tubes.

 

Our Monel K500 Pipes can be reinforced further by cold rolling prior to compressive loading. These Monel K500 Seamless Pipes are vital for obtaining a water supply quench from the heating rate without delay for optimal ageing resistance and maximal softness. Our Monel K500 Welded Tubes have non-magnetic qualities and are used in aircraft instrument systems. Standard commercial processes can be used to construct these Monel K500 EFW Pipes.

 

Even at temperatures as low as fluid hydrogen, there is no ductile-to-brittle conversion, making our Monel K500 Pipes suitable for cryogenic applications. Heavy machining of these Monel K500 Square Tubes is best performed when the material is annealed or hot-worked and tempered. Monel K500 Pipes and Tubes can be purchased at a reasonable cost. These are made to withstand corrosion and acid attacks. These perform well in corrosive environments in a variety of applications. These pipes and tubes are stronger and more robust. They have a seamless and flawless finish, as well as exact, optimal thicknesses and proportions.

Throughout the manufacturing process, our pipes and tubes are subjected to a variety of destructive and non-destructive testing. Our professionals inspect the functionality and specifications of products to ensure error-free shipment.

K500 alloy corrosion resistant Pipes

Monel Alloy K500 corrosion resistant Pipes

 

SPECIFICATION OF Monel K500 PIPES

Seamless Pipe & Tube: ASTM B165 / ASME SB165

Welded Pipe: ASTM B725 / ASME SB725

Welded Tube:ASTM B730 / ASME SB730

Pipe Outside Diameter: 6.00 mm OD up to 914.4 mm OD, Sizes up to 24″ NB available Ex-stock, OD Size Steel Tubes                                        

Tube Outside Diameter: 1/8″ OD TO 2″OD 3MM OD TO 38 MM OD

Thickness Range: 1MM TO 3 MM 0.028 TO 0.156 IN, SCH 5, SCH10, SCH 40, SCH 80, SCH 80S, SCH 160, SCH XXS

Type: Seamless / ERW / Welded

Form: Round Pipe & Tube

Length: Single Random, Double Random & Required Length

End: Plain End, Beveled End, Threaded

CHEMICAL COMPOSITION OF Monel K500 PIPES

Grade C Mn Si S Cu Fe Ni Cr
Monel K500
0.30 max
2.00 max
0.50 max 0.024max
28.00 – 34.00
2.50 max
63.00 min
14.00 – 17.00

Monel K500 TUBES MECHANICAL PROPERTIES

Element Density Melting Point Tensile Strength Yield Strength (0.2%Offset) Elongation
Monel K500 8.8 g/cm3 1350 °C (2460 °F) Psi – 80,000 , MPa – 550 Psi – 35,000 , MPa – 240 40 %

GNEE Group Factory Environment

Monel K500 corrosion resistant Pipes

Monel Alloy K500 corrosion resistant PipesMonel Alloy K500 corrosion resistant Pipes

Monel Alloy K500 corrosion resistant Pipes

FAQ

Q: What are the advantages of your company?
A: We have many professionals, technicians, more competitive prices and the best after-sales service than other stainless steel companies.
Q: How many countries have you exported to?
A: Exported to more than 50 countries, mainly from the United States, the United Kingdom, Kuwait, Egypt, Turkey, Jordan, India, etc.
Q: Can you provide samples?
Answer: Yes. As long as you contact us, we can provide free small samples in stock. Customized samples will take about 5-7 days.

 

Hot Tags: Monel Alloy K500 corrosion resistant Pipes, China Monel Alloy K500 corrosion resistant Pipes suppliers, alloy tempering, dimensional stability alloy, tensile strength alloy, alloy purpose, alloy annealing, high strength alloy

Send Inquiry

whatsapp

Phone

E-mail

Inquiry