Monel 405
video

Monel 405

Industry Names
• Monel R-405
• Alloy 405
• Nickel 405
Material
• Exotic
• Specialty Steel
Specifications
• ASTM B127 QQ-N-281 (Sheet)
• ASTM B164 QQ-N-281 (Bar)
• UNS N04405
Send Inquiry
Chat Now

As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.

Product Introduction

Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of monel 405 in China. If you're going to wholesale high quality monel 405 made in China, welcome to get free sample from our factory. Good service and reasonable price are available.

 

Monel 405 information
 

GNEE STEEL monel 405 video

GNEE Monel 405 Equivalent grade

  • UNS N04405

    W.Nr.2.4363

    ASTM B164

    ASME SB164

    QQ-N-281

Form

Standard

Metal Type

UNS N04405

Bar

ASTM B164 QQ-N-281

Wire

 

Sheet

ASTM B127 QQ-N-281

Plate

ASTM B127 QQ-N-281

Fitting

 

Forging

ASTM B564

Weld Wire

 

Weld Electrode

FM 190/ ENiCu-7

Monel 405 chemical composition
 

 

The chemical composition nickel alloy 405 is outlined in the following table.

Element Content (%)
Nickel+Cobalt, Ni+Co 63
Copper, Cu 28-34
Iron, Fe 2.5
Manganese, Mn 2
Silicon, Si 0.5
Carbon, C 0.3
Sulfur, S 0.025-0.06

 

Monel R405 is the free machining version of Monel 400. It is a nickel-copper alloy with a controlled amount of sulfur added to provide sulfide inclusions that act as chip breakers during machining. Like Monel 400, alloy R-405 is resistant to sea water and steam at high temperatures as well as to salt and caustic solutions. Monel R405 is a solid solution alloy that can only be hardened by cold working. This nickel alloy exhibits characteristics like good corrosion-resistance, good weldability and high strength. A low corrosion rate in rapidly flowing brackish or seawater combined with excellent resistance to stress corrosion cracking in most freshwaters, and its resistance to a variety of corrosive conditions led to its wide use in marine applications and other non-oxidizing chloride solutions. This nickel steel alloy is particularly resistant to hydrochloric and hydrofluoric acids when they are de-aerated. As would be expected from its high copper content, alloy R-405 is rapidly attacked by nitric acid and ammonia systems.

 

GNEE Monel 405 Parameter
 

 

Condition

Tensile (ksi)

.2% Yield (ksi)

Elongation %

Hardness Brinell (3000 kg)

Hardness Rockwell B

Annealed

70-85

25-40

50-35

110-140

60-76

Hot-Finished

75-90

35-60

45-30

130-170

72-86

Cold-Drawn, As-Drawn

85-115

50-105

35-15

160-245

85-23C

 

GNEE Monel 405 Application
 

 

  • Automatic screw machine application
  • Marine engineering
  • Chemical and hydrocarbon processing equipment
  • Gasoline and freshwater tanks
  • Crude petroleum stills
  • De-aerating heaters
  • Boiler feed water heaters and other heat exchangers
  • Valves, pumps, shafts, fittings, and fasteners
  • Industrial heat exchangers
  • Chlorinated solvents
  • Crude oil distillation towers

 

GNEE Monel 405 Feature
 

 

Characteristics are essentially the same as those of Monel 400 such as:
• Good machinability and is recommended for use with automatic screw machines
• Resistant to seawater and steam at high temperatures
• Excellent resistance to rapidly flowing brackish water or seawater
• Excellent resistance to stress corrosion cracking in most freshwaters
• Particularly resistant to hydrochloric and hydrofluoric acids when they are de-aerated
• Offers some resistance to hydrochloric and sulfuric acids a modest temperatures and concentrations, but is seldom the material of choice for these acids
• Excellent resistance to neutral and alkaline salt
• Resistance to chloride induced stress corrosion cracking
• High resistance to alkalis
 

Our Company
 

 

Monel 405

38000㎡ workshop and 200+ emplovees to meet your huge demands.

 

GNEE MONEL 405 Packing & Delivery
 

GNEE MONEL 405 Packing & Delivery

Monel 405

 

Customer Visit
 

 

Monel 405

Gnee exports steel to over 70 countries and collaborates with more than 600 companies worldwide

 

FAQ
 

 

Q: What are the advantages of your company ?

A: We have many professionals, technical personnel, more competitive prices and best after-dales service than other stainless steel companies.

Q: Can you provide sample ?

A: Yes. We can provide the small samples in stock for free, as long as you contact us.Customized samples will take about 5-7 days.

Q:Can you send samples?

A:Of course, we can send samples to all parts of the world, our samples are free, but customers need to bear the courier costs.

 

Hot Tags: monel 405, China monel 405 suppliers, alloy annealing, alloy technology, alloy financing, alloy commerce, alloy sales, alloy marketing

Send Inquiry

whatsapp

Phone

E-mail

Inquiry