Monel 405 Alloy Coil
As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.
- Send E-mail: ss@gneesteel.com
Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of monel 405 alloy coil in China. If you're going to wholesale high quality monel 405 alloy coil made in China, welcome to get free sample from our factory. Good service and reasonable price are available.
Introduction to Monel 405 Alloy Plate:
Monel 405 is a nickel-copper alloy renowned for its exceptional corrosion resistance in a variety of environments, particularly in reducing conditions. It is essentially a solid-solution alloy that offers improved corrosion resistance compared to Monel 400, specifically in reducing media such as sulfuric acid and hydrofluoric acid. Monel 405 alloy plate finds widespread applications across industries where resistance to corrosive environments is essential.

Key Features:
Corrosion Resistance: Seawater, sulfuric acid, hydrofluoric acid, and other reducing media are just a few of the conditions in which Monel 405 alloy plate exhibits exceptional resistance to corrosion. This qualifies it for uses when exposure to caustic substances is unavoidable.
Better Performance: Monel 405 performs better than Monel 400 in terms of corrosion resistance, especially in reducing situations. Because of its solid-solution composition, which offers enhanced resistance to corrosive assault, it is the perfect option for demanding applications where dependability is crucial.
Mechanical capabilities: Even at high temperatures, Monel 405 maintains its strong mechanical capabilities, including as high strength and ductility. Because of these qualities, it may be used for equipment and structural parts that are subjected to significant mechanical loads and stress.

Applications:
Chemical Processing: A wide range of chemical processing industries employ Monel 405 alloy plate, especially those with sulfuric acid, hydrofluoric acid, and other reducing media present. Reactors, vessels, and other equipment that requires corrosion resistance use it.
Maritime Engineering:Applications for Monel 405 in maritime engineering include heat exchangers, marine fittings, and seawater piping systems. It is appropriate for components exposed to maritime settings due to its resistance to corrosion in seawater.
Oil and Gas: Tubing systems, valves, and downhole equipment in the oil and gas sector are made of Monel 405 alloy plate. It is a good fit for offshore and subsea applications due to its mechanical qualities and resistance to corrosion.
Specifications:
| Specification | Description |
|---|---|
| Thickness | 0.1 mm - 10 mm |
| Width | 100 mm - 2000 mm |
| Length | Customized |
| Surface Finish | Cold Rolled, Hot Rolled, Acid Pickled, Bright Surface |
| Material | Monel 405 Alloy |
| Strength | ≥ 480 MPa |
| Tensile Strength | ≥ 550 MPa |
| Yield Strength | ≥ 240 MPa |
| Density | 8.80 g/cm³ |
| Melting Point | 1300-1350°C |
| Corrosion Resistance | Excellent resistance to seawater, sulfuric acid, hydrofluoric acid, etc. |
| Typical Applications | Chemical Processing, Marine Engineering, Oil and Gas |
| Manufacturing Standards | ASTM B127, ASME SB127 |
In summary, Monel 405 alloy plate offers exceptional corrosion resistance and mechanical properties, making it a preferred choice for critical applications across chemical processing, marine engineering, and oil and gas industries.