Incoloy Alloy 330 Pipe
video

Incoloy Alloy 330 Pipe

As a leading Chinese Incoloy pipe supplier, AEETHER manufactures and produces different sizes of Incoloy 330 welded pipes & tubes.INCOLOY alloy 330 (UNS N08330 / W.Nr. 1.4886) is an austenitic alloy with good high-temperature strength and corrosion resistance. It has a solid solution composition and is not hardenable by heat treatment. Its high nickel and chromium provide good resistance to oxidation and carburization. Its oxidation resistance is enhanced by the silicon content.
Send Inquiry
Chat Now

As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.

Product Introduction

Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of incoloy alloy 330 pipe in China. If you're going to wholesale high quality incoloy alloy 330 pipe made in China, welcome to get free sample from our factory. Good service and reasonable price are available.

 

Incoloy Alloy 330 is a nickel-chromium-molybdenum alloy that exhibits excellent high-temperature strength and oxidation resistance. It also demonstrates good resistance to a wide range of corrosive environments, including sulfuric and phosphoric acids. Incoloy Alloy 330 pipe is commonly used in heat exchangers, chemical processing, and other industrial applications where high-temperature strength and corrosion resistance are required.

Physical Properties

The following table discusses the physical properties of INCOLOY alloy 330.

Properties Metric Imperial
Density 8.08 gm/cm3 0.292 lb/in3

Mechanical Properties

The mechanical properties of INCOLOY alloy 330 are tabulated below.

Properties Metric Imperial
Tensile strength(annealed) 600 MPa 87 ksi
Yield strength(annealed) 280 MPa 40.6 ksi
Elongation at Break 45% 45%

 

Incoloy Alloy 330 pipeIncoloy Alloy 330 pipeIncoloy Alloy 330 pipe